MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik 2-Propylheptanol
Categories: Fluid

Material Notes: CAS No: 1042-59-8

2-Propylheptanol is classified as irritating to eyes and skin.

Application: 2-Propylheptanol is predominantly used as alcohol component in plasticizer manufacturing.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.8324 g/cc0.03007 lb/in³ASTM D4052
Viscosity 15.3 cP15.3 cPdynamic; ASTM D445
Molecular Weight 158.3 g/mol158.3 g/mol
Vapor Pressure 0.000200 bar0.150 torr
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 0.10<= 0.10[mg KOH/g]; DIN EN ISO 2114
 
Thermal PropertiesMetricEnglishComments
Melting Point <= -100 °C<= -148 °F
Distillation Temperature 205 - 220 °C
@Pressure 0.1013 MPa
401 - 428 °F
@Pressure 14.69 psi
ASTM D1078
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.43691.4369ASTM D1045
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.10 %<= 0.10 %DIN 51 777
 
Descriptive Properties
Color<10 Pt/lAPHA, Hazen, ASTM D1209
Content>99.5%Ecanol Isomers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIL961 / 197165

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.