MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite Methylon 75108 Coating Intermediate
Categories: Polymer; Thermoplastic

Material Notes: DESCRIPTION: Methylon 75108 is a coating intermediate containing a mixture of the allyl ethers of mono-, di-, and trimethylol phenols.

APPLICATION: Methylon 75108 is used as a metal coating intermediate; in coatings and linings for containers and chemical processing or handling equipment where resistance to chemicals, heat, humidity, impact and abrasion are required.

Other applications include:

  • Drum, pail, and can linings
  • Food containers
  • Tank cars
  • Air conditioning equipment
  • Water tanks
  • Appliances
  • Chemical tanks
  • Process equipment
  • Metal goods

FEATURES:

  • Outstanding resistance to alkalis, acids, soaps, detergents, solvents, salts, oxidizing agents, salt spray, and other corrosive materials.
  • Extremely tough and resistant to marring and abrasion.
  • Excellent adhesion to metals (iron, steel, copper, brass, aluminum, magnesium).
  • Excellent adhesion to glass and many plastics.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.16 g/ccDCT 5075
Water Absorption <= 3.0 %Karl Fischer; DCT 4021A
pH 6.5DCT 4064A
Viscosity 3000 cP
@Temperature 25.0 °C
DCT 4003F
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 10G-H; DCT 4075A
 
Descriptive Properties
Non Volatile (%)86.5125°C, 2.5 g, 45 min; DCT 4064A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials TIVAR™ Extended Wear UHMW-PE, Premium Glass-filled, Partially Cross-linked
Sumitomo Bakelite Sumikon® PM-6430 Glass-Filled Phenolic, Compression Grade
Petromont 3100 High Density Polyethylene Resin
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M77HS Moldable
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M33 Moldable

PSUMIT170 / 193975

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.