System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Teknor Apex Chemlon® 190 Polyamide 66
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
Material Notes:
Availability: Asia Pacific, Europe, North America.
Form : pellets.
Processing method: injection molding
Features: high viscosity
Uses: coating applications, rods, tubing, wire jacketing
Appearance: natural color.
Information provided by Teknor Apex.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.14
g/cc
ASTM D792
Mechanical Properties
Original Value
Comments
Tensile Strength
12500
psi
ASTM D638
Elongation at Break
60 %
ASTM D638
Flexural Strength
16500
psi
@ 73°F; ASTM D790
Flexural Modulus
420000
psi
@Temperature 22.8 °C
ASTM D790
Izod Impact, Notched
1.60
ft-lb/in
@Temperature 22.8 °C
ASTM D256
Thermal Properties
Original Value
Comments
Melting Point
500
°F
Flammability, UL94
V-0
@Thickness 0.635 mm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
PlastiComp Complet® LCF40 - PP Homopolymer Polypropylene, 40% Long Carbon Fiber Reinforced
RTP Company RTP 399 X 91042 Polycarbonate (PC), Thermally Conductive - Electrically Insulative
RTP Company RTP 387 Polycarbonate (PC), Carbon Fiber
Bohler-Uddeholm UDDEHOLM ORVAR® SUPERIOR (Premium AISI H13) Hot Work Tool Steel
Thermal Transfer Composites PRIMEX ULTRA™ MCT-587™ Aluminum Silicon Carbide Composite, Reinforced
PTEKNN9706 / 231060
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.