MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PPM R020 Polypropylene, Random Copolymer for Medical Grade
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Polypropylene PPM R020 is a random copolymer polypropylene with a Melt Flow Index of 1.8 g/10 min specially developed for the extrusion blow molding of medical containers and medical devices, to the exclusion of implants.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.902 g/ccISO 1183
Bulk Density 0.525 g/ccISO 1183
Melt Flow 1.8 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 82ISO 2039-2
Tensile Strength, Yield 26.0 MPaISO 527-2
Elongation at Yield 10 %ISO 527-2
Tensile Modulus 1000 MPaISO 527-2
Flexural Modulus 900 MPaISO 179
Izod Impact, Notched (ISO) 6.00 kJ/m²ISO 180
Charpy Impact, Notched 8.00 kJ/m²ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 149 °CISO 3146
Vicat Softening Point 67.0 °C
@Load 5.10 kg
50°C per hour; ISO 306
 130 °C
@Load 1.02 kg
50°C per hour; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPM H350 Polypropylene, Homopolymer Medical Grade
Total PPM R021 Polypropylene, Random Copolymer for Medical Grade
Ensinger TECAPRO™ MT Medical Grade Polypropylene (PP)
Total PPM H250 Polypropylene, Homopolymer Medical Grade
Avient Trilliant™ HC HC5220-0040 RS Natural Polypropylene

PTOTAL875 / 130600

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.