MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Tisan TISOPLEN® 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include
  • Low density
  • Low moisture intake
  • High impact resistance
  • Excellent chemical resistance
  • Electrical isolation
  • High performance/affordable price
  • Easy processability
Mineral filled TISOPLEN compounds have a long lasting thermal-dimensional stability, increased mechanical and hardness characteristics, decreased mold shrinkage and improved surface appearance. Glass fiber reinforcement will impart high tensile strength and impact resistance and yield improvements in thermal characteristics of TISOPLEN products. Excellent resistance to weak acids, weak alkalis, and strong alkalis. Good resistance to strong acids and alcohols. Medium resistance to hydrocarbons and engine fuels. Weak resistance to organic solvents.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/ccISO 1183
Moisture Absorption 0.010 %ISO 62
Linear Mold Shrinkage 0.014 cm/cm
Melt Flow 15 g/10 minISO 1133
Ash 15 %ISO 3451
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 66ISO 868
Tensile Strength at Break 27.0 MPaISO 527-2
Tensile Strength, Yield 38.0 MPaISO 527-2
Elongation at Break 3.0 %ISO 527-2
Elongation at Yield 5.0 %ISO 527-2
Modulus of Elasticity 2.50 GPaISO 527-2
Izod Impact, Notched (ISO) 4.50 kJ/m²ISO 180
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 600 VTS EN 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °C
Vicat Softening Point 130 °CISO 306
Heat Distortion Temperature 135 °CISO 75-2
Flammability, UL94 V-0
 
Processing PropertiesOriginal ValueComments
Feed Temperature 70.0 °C
Rear Barrel Temperature 190 - 210 °CAft-1. Region Temperature
Middle Barrel Temperature 190 - 210 °CMid-2. Region Temperature
Front Barrel Temperature 190 - 210 °CPre-3. Region Temperature
Nozzle Temperature 200 °C
Melt Temperature 170 - 190 °C
Drying Temperature 80.0 °CPredrying Temperature
Dry Time 1 hourPredrying Time
 
Descriptive Properties
Block Temperature45°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Synres® PP HFR005 Polypropylene
Tipco Tipcolene® FPT 20 FR VO LTHA - UL94-V0 Flame Retardant, 20% Talc Polypropylene Homopolymer, Long Term Heat Stability
Tipco Tipcolene® FPT 20 FR VO PPC - UL94-V0 Flame Retardant, 20% Talc Polypropylene Copolymer
Tipco Tipcolene® FX 6000 - UL94-V0 Flame Retardant & Mineral Reinforced Polypropylene Copolymer
Tisan TISOPLEN® 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Copolymer Polypropylene

PTIS038 / 79473

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.