MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Gromax CCP PET 9130-200 30% Glass Filled
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 30% Glass Reinforced

Material Notes: Product Description: PET glass/mineral 30% reinforced injection molding grade.

Characteristics:

  • Excellent electrical property
  • Excellent mechanic and chemical property
  • Excellent weatherability
  • Excellent wear property
  • Excellent moldability
  • High resistance to fuels, oil, fats and many solvents
  • Low warp age

    Information provided by Gromax Enterprises Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.68 g/cc1.68 g/ccASTM D792
Moisture Absorption 0.0500 %
@Time 86400 sec
0.0500 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage  0.0010 - 0.0030 cm/cm
@Thickness 1.60 mm
0.0010 - 0.0030 in/in
@Thickness 0.0630 in
horizontal; ASTM D955
 0.0050 - 0.010 cm/cm
@Thickness 1.60 mm
0.0050 - 0.010 in/in
@Thickness 0.0630 in
vertical; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 113 MPa16400 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Flexural Strength 175 MPa25400 psiASTM D790
Flexural Modulus 9.81 GPa1420 ksiASTM D790
Izod Impact, Notched >= 0.883 J/cm
@Thickness 6.35 mm
>= 1.65 ft-lb/in
@Thickness 0.250 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Surface Resistance 1.00e+13 ohm1.00e+13 ohmASTM D257
Dielectric Constant 3.8
@Frequency 60 Hz
3.8
@Frequency 60 Hz
ASTM D150
Dielectric Strength 23.0 kV/mm
@Thickness 2.00 mm
584 kV/in
@Thickness 0.0787 in
ASTM D149
Dissipation Factor 0.011
@Frequency 60 Hz
0.011
@Frequency 60 Hz
ASTM D150
Arc Resistance 100 sec100 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 µm/m-°C11.1 µin/in-°FASTM D696
Melting Point 254 °C489 °FDSC
Deflection Temperature at 0.46 MPa (66 psi) 247 °C477 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 230 °C446 °FASTM D648
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 250 - 270 °C482 - 518 °F
Nozzle Temperature 260 - 280 °C500 - 536 °F
Mold Temperature 80.0 - 140 °C176 - 284 °Fsuitable temperature 90-120°C
Injection Pressure 50.0 - 120 MPa7250 - 17400 psi
Hold Pressure 30.0 - 80.0 MPa4350 - 11600 psi
Back Pressure 0.000 - 0.300 MPa0.000 - 43.5 psi
Screw Speed 100 - 200 rpm100 - 200 rpmto be chosen in such a way that plasticizing time is just within cooling time
 
Descriptive Properties
Injection Ratemiddle-fast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chengdu Polyster H3030 Thermoplastic Polyether-ester Elastomer (TPEE)
Gromax CCP PET 9130-104 30% Glass Filled
Overview of materials for Nylon 6, Glass Filled, Impact Grade
Gromax CCP PBT 4830-BK 30% Glass Fiber Filled
Celanese Zytel® 74G33W NC010 PA66+PA6-GF33

PGROM047 / 147860

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.