MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Norplex-Micarta EnableX™ Cotton Phenolic Prepreg System
Categories: Polymer; Thermoset; Phenolic

Material Notes: EnableX™ allows continuous fiber pre-preg to be co-cured in a multi-material molding system to produce near net shapes. Building upon the predictability of continuous fiber reinforced pre-preg, EnableX™ materials are ppecifically designed for compression molding and tested to ensure compatibility. The in-house laboratory and development capabilities allow for new concepts to be prototyped, or specific datasets to be developed to support specific design criteria.

Features:

  • Superior specific strength and stiffness
  • Inherent chemical resistance
  • Excellent dielectric properties
  • Self-lubricating and low wear
  • Low FST generation

Reported property data is for prepreg pressed into flat sheet.

Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 13.0 ksi90° Orientation; ASTM D3039
 14.0 ksi0° Orientation; ASTM D3039
Tensile Modulus 1.34e+6 psi90° Orientation; ASTM D3039
 1.51e+6 psi0° Orientation; ASTM D3039
Shear Modulus 1360 ksi±45° Orientation, In-plane; ASTM D3518
Shear Strength 4.00 ksi0° Orientation, Short Beam; ASTM D2344
 4.00 ksi90° Orientation, Short Beam; ASTM D2344
 12.0 ksi±45° Orientation, In-plane; ASTM D3518

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNORPM254 / 280532

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.