MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Medium-leaded brass, UNS C34000, OSO25 Temper wire
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Fair to excellent corrosion resistance. Fabricated by blanking, heading and upsetting, machining, piercing and punching, roll threading and knurling, stamping.

Applications: couplings, free machining screws and rivets, gears, nuts, or tire valve stems.

Test specimen: wire - 2mm diameter.

Key Words: 340 brass, CZ118, ISO CuZn35Pb1, CEN CW600N
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.47 g/cc0.306 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 345 MPa50000 psi
Elongation at Break 50 %50 %In 50 mm
Modulus of Elasticity 105 GPa15200 ksi
Poissons Ratio 0.3460.346
Machinability 60 %60 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 39.0 GPa5660 ksi
Shear Strength 235 MPa34100 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000660 ohm-cm0.00000660 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.3 µm/m-°C
@Temperature 20.0 - 300 °C
11.3 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 115 W/m-K
@Temperature 20.0 °C
798 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 885 - 925 °C1630 - 1700 °F
Solidus 885 °C1630 °F
Liquidus 925 °C1700 °F
Annealing Point 427 - 649 °C800 - 1200 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 425 - 650 °C797 - 1200 °F
Recrystallization Temperature 288 °C550 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 62.5 - 66.5 %62.5 - 66.5 %
Iron, Fe <= 0.10 %<= 0.10 %
Lead, Pb 0.80 - 1.4 %0.80 - 1.4 %
Other, total <= 0.50 %<= 0.50 %
Zinc, Zn 34 %34 %As remainder

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Medium-leaded brass, UNS C34000, H00 Temper wire
Medium-leaded brass, UNS C34000, H01 Temper wire
Medium-leaded brass, UNS C34000, H02 Temper wire
Tin-Bearing Copper Nickel, UNS C72500, Quarter Hard flat products
Medium-leaded brass, UNS C34000, H02 Temper flat products

MC34000c1 / 11195

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.