MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
LG Chemical NPG Flake Neopentyl Glycol  (discontinued **)
Categories: Other Engineering Material

Material Notes: NPG is a diol with two hydroxyl groups located in the 1,3-position on the primary carbon atom. Additionally, it has two methyl groups instead of the usual two hydrogen atoms on the a-carbon atom. Its unique structure is responsible for allowing rapid esterification, high chemical and thermal stability of NPG as well as high crystalline and weatherability.

Applications: Powder Coating Resins, Alkyd Coating Resins, Fiber Glass Reinforced Resins, Polyester Polyols Plasticizer

CAS No. 126-30-7

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/cc
Molecular Weight 104.15 g/mol
Vapor Pressure 3.00 torr
@Temperature 20.0 °C
Vapor density: 2.1
 
Thermal PropertiesOriginal ValueComments
Boiling Point 210 °C
@Pressure 0.101 MPa
Flash Point 103 °C
Ignition Temperature 399 °CAutoignition
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 3.0 %ASTM E203
 
Descriptive Properties
Acidity<0.01%
Color10 APHA50% in H2O, ASMT D1209
Hydroxyl functionality2
Hydroxyl Number1050-1090 KOH mg/g
Purity>99.2%Gas Chro.
Solubility520 g/100gin H2O (20°C)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tungsten Silicide, WSi2

PLAY366 / 148376

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.