MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Azoty Tarnow™ TARNOFORM 400 POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Easy flowing, fast cycling injection molding grade for manufacturing of thin-wall details

Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccISO 1183
Linear Mold Shrinkage 0.028 cm/cm
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 114ISO 2039-2
Ball Indentation Hardness 140 MPa358 N; ISO 2039-1
Tensile Strength, Yield 68.0 MPaISO 527
Elongation at Break 45 %ISO 527
Flexural Strength 64.0 MPaISO 178
Izod Impact, Notched (ISO) 0.700 J/cm²1A; ISO 180
Charpy Impact, Notched 0.600 J/cm²1eA; ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohmIEC 60093
Dielectric Constant 3.9
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 25.0 kV/mmIEC 60243
Dissipation Factor 0.0085
@Frequency 1e+6 Hz
IEC 60250
Arc Resistance 1.9 sec
Comparative Tracking Index 600 VIEC 112
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.48 J/g-°C
Melting Point 167 °C10°C/min.; ISO 3146
Maximum Service Temperature, Air 100 °C
Deflection Temperature at 1.8 MPa (264 psi) 115 °CISO 75
Vicat Softening Point 150 °C50 N; ISO 306
Flammability, UL94 HB
@Thickness 3.20 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 230 °CBarrel temperature
Mold Temperature 60.0 - 120 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röchling Polystone® M Flame Retardant PE-UHMW
Polikim ULPOLEN® 1000 UHMWPE, Flame Retardant
Celanese Hostaform® C 13031 POM, Unfilled
Celanese Hostaform® C 13021 POM, Unfilled
Celanese GUR® 4120 PE-UHMW, Unfilled

PZAK033 / 72872

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.