MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Entec Enflex® EA5790A Styrenic Block, TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Product Description: 90 Shore A TPE available in black and natural offering high heat performance with excellent oil and fluid resistance. This grade also exhibits high strength, good flexibility and resiliency. Intended for injection molding and extension processing. Designed for user the hood applications such as gaskets, grommets, seals, slugs where high heat and oil resistance is required.

Availability: North America

Features: Alcohol Resistant; Detergent Resistant; Good Adhesion; Good Colorability; Good Flexibility; Good Processability; High Elasticity; High Heat Resistance; High Strength; Low Compression Set; Oil Resistant; Ozone Resistant; Recyclable Material; Resilient; Soft; Solvent Resistant; UV Resistant

Uses: Automotive Applications; Automotive Under the Hood; Gaskets; Grommets; Plugs; Seals

Appearance: Black; Natural Color

Processing Method: Extrusion; Injection Molding

Information provided by Entec Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccASTM D792
Melt Flow 2.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90
@Time 10.0 sec
Injection Molded; ASTM D2240
Hardness, Shore D 35
@Time 10.0 sec
Injection Molded; ASTM D2240
Tensile Strength at Break 1600 psiASTM D412
Elongation at Break 480 %ASTM D412
Flexural Modulus 13.2 psi1% Tangent; ASTM D412
Tear Strength 325 pliASTM D624
Compression Set 33 %
@Temperature 22.8 °C,
Time 79200 sec
ASTM D395B
 65 %
@Temperature 100 °C,
Time 79200 sec
ASTM D395B
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -30.0 °FASTM D746
 
Processing PropertiesOriginal ValueComments
Processing Temperature 355 - 430 °FHopper, Extrusion
Rear Barrel Temperature 390 - 430 °F
Middle Barrel Temperature 430 - 465 °F
Front Barrel Temperature 430 - 465 °F
Nozzle Temperature 430 - 465 °F
Zone 1 410 - 445 °F
Zone 3 410 - 445 °F
Zone 5 410 - 445 °F
Adapter Temperature 410 - 445 °F
Die Temperature 410 - 445 °F
Melt Temperature 410 - 445 °FExtrusion
 430 - 445 °FInjection
Mold Temperature 50.0 - 120 °FInjection
Drying Temperature 175 - 212 °FInjection
 175 - 212 °FExtrusion
Injection Pressure 750 - 1300 psi
Cushion 0.200 - 0.500 in
Screw Speed 50 - 200 rpmInjection
 100 - 200 rpmExtrusion
 
Descriptive Properties
Dynamic Service Temperature338°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENTB595 / 311288

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.