MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Hostaform® S 9243 XAP2 ™ POM, Impact Modified
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Impact Modified

Material Notes: POM copolymer, modified
It is normally not necessary to dry HOSTAFORM. However, should there be surface moisture (condensate) on the molding compound as a result of incorrect storage, drying is required. A circulating air drying cabinet can be used for this purpose if the granul
The product can then be stored in standard conditions until processed.

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.33 g/ccISO 1183
Water Absorption at Saturation 1.0 %ISO 62
Linear Mold Shrinkage, Flow 0.019 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.018 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 44.0 MPa50mm/min; ISO 527-2/1A
Elongation at Break 40 %50mm/min; ISO 527-2/1A
Elongation at Yield 9.0 %50mm/min; ISO 527-2/1A
Tensile Modulus 1950 MPa1mm/min; ISO 527-2/1A
Flexural Modulus 1850 MPaISO 178
Charpy Impact Unnotched NBISO 179/1eU
 200 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 15.0 kJ/m²ISO 179/1eA
 9.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
Tensile Creep Modulus, 1 hour 1700 MPaISO 899-1
Tensile Creep Modulus, 1000 hours 950 MPaISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Constant 3.8
@Frequency 1e+6 Hz
IEC 60250
 3.8
@Frequency 100 Hz
IEC 60250
Dissipation Factor 0.0030
@Frequency 100 Hz
IEC 60250
 0.0060
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 120 µm/m-°CISO 11359-2
Melting Point 166 °CISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °CISO 75-1, -2
Vicat Softening Point 130 °CB50 (50°C/h 50N); ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 - 30.0 °Chopper
 60.0 - 80.0 °Ccavity
Feed Temperature 60.0 - 80.0 °C
Zone 1 170 - 180 °C
Zone 2 180 - 190 °C
Zone 3 190 - 200 °C
Zone 4 190 - 200 °C
Die Temperature 190 - 200 °C
Melt Temperature 190 - 200 °C
Drying Temperature 100 - 120 °C
Dry Time 3 - 4 hour
Moisture Content 0.15 %Necessary low maximum
Injection Pressure 8700 - 17400 psi
Hold Pressure 8700 - 17400 psi
Back Pressure <= 290 psi
Screw Speed 70 rpm
@Diameter 55.0 mm
 100 rpm
@Diameter 40.0 mm
 150 rpm
@Diameter 25.0 mm
Hot-Working Temperature 190 - 200 °C
 
Descriptive Properties
Injection moldingYes
Injection speedslow-medium
Melt volume rate (MVR), cm³/10min4
MVR test load, kg2.16
MVR test temperature, °C190
Processing conditions acc. ISO9988-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Hostaform® S 9243 XAP2™ LS POM, Impact Modified
Celanese Hostaform® S 9364 POM, Impact Modified
Celanese Hostaform® S 9243 XAP² ™ POM, Impact Modified
Celanese Hostaform® S 9243 XAP² ™ LS POM, Impact Modified
Celanese Hostaform® S 9243 Impact Grade Acetal Copolymer

PHCS397 / 123812

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.