MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Apec® DP9-9351 High-Heat Polycarbonate, General Purpose  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, High Heat

Material Notes: Information provided by Bayer Corporation, Plastics Division

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This product was discontinued prior to the separation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccASTM D792
Water Absorption 0.20 %24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0080 - 0.0090 cm/cmASTM D955
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 330 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 84ASTM D785
Hardness, Rockwell R 127ASTM D785
Tensile Strength, Ultimate 62.0 MPaASTM D638
Tensile Strength, Yield 66.0 MPaASTM D638
Elongation at Break 80 %ASTM D638
Elongation at Yield 6.0 %ASTM D638
Tensile Modulus 2.20 GPaASTM D638
Flexural Yield Strength 86.0 MPaASTM D790
Flexural Modulus 2.28 GPaASTM D790
Izod Impact, Notched 1.10 J/cm
@Thickness 3.17 mm
ASTM D256
Izod Impact, Unnotched NBASTM D256
 NB
@Temperature -40.0 °C
ASTM D256
Impact Test 66.0 J
@Thickness 3.20 mm
Instrumented Impact, Total Energy; 3.2 mm thick, 15 mph, 3 in. clamp, 0.5 in. dart; ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+16 ohm-cmASTM D257
Surface Resistance >= 1.00e+16 ohmASTM D257
Dielectric Constant 2.9
@Frequency 60 Hz
ASTM D150
 2.9
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength >= 16.0 kV/mm
@Thickness 3.17 mm
ASTM D149
Dissipation Factor 0.0010
@Frequency 60 Hz
ASTM D150
 0.010
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 120 - 180 sec
@Thickness 3.00 mm
UL Rating PLC 5 (120-180 sec)
Comparative Tracking Index 400 - 600 V
@Thickness 3.00 mm
UL Rating PLC 1 (400-600 V)
Hot Wire Ignition, HWI 30 - 60 sec
@Thickness 1.50 mm
UL Rating PLC 2 (30-60 sec)
High Amp Arc Ignition, HAI <= 15 arcs
@Thickness 1.50 mm
UL Rating PLC 4 (<15 arcs)
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/min
@Thickness 3.00 mm
UL Rating PLC 2 (25.4-80 mm/min.)
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Thermal Conductivity 0.210 W/m-KASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 174 °C
@Thickness 3.20 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 162 °C
@Thickness 3.17 mm
ASTM D648
Vicat Softening Point 185 °CRate B; ASTM D1525
UL RTI, Electrical 150 °C
@Thickness 1.50 mm
UL746B
UL RTI, Mechanical with Impact 130 °C
@Thickness 1.50 mm
UL746B
UL RTI, Mechanical without Impact 150 °C
@Thickness 1.50 mm
UL746B
Flammability, UL94 HB
@Thickness 1.50 mm
 HB
@Thickness 1.50 mm
Oxygen Index 24 %ASTM D2863
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.572ASTM D542
Haze 1.0 %
@Thickness 3.17 mm
ASTM D1003
Transmission, Visible 88 %
@Thickness 3.20 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Processing Temperature 315 - 340 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical Lupoy 1201-22 Polycarbonate Resin
Covestro Apec® HT KU 1-9351 High-Heat Polycarbonate
Covestro Apec® HT KU 1-9353 High-Heat Polycarbonate, UV-Stabilized
Covestro Apec® HT KU 1-9354 High-Heat Polycarbonate
Covestro Apec® DP9-9331 High-Heat Polycarbonate, General Purpose

PB1A05 / 26387

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.