MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Teresstic M Series 32LT
Categories: Fluid; Lubricant

Material Notes: The Teresstic M Series of products is the latest addition to the family of Teresstic turbine lubricant products, long recognized for their high quality and reliability. Teresstic M Series are designed for use in Mitsubishi Heavy Industries (MHI) Gas and Steam turbines for both light and heavy-duty applications. Teresstic M Series oils are formulated with carefully selected premium basestocks and selected additives, including antioxidants, rust, and corrosion inhibitors and anifoam agents. The Teresstic M Series of products are designed to provide a reliable lubricant solution for MHIs newly released stringent performance requirements for gas and steam  turbines. These products also meet the strict performance requirements for GE steam and light duty gas turbines. Teresstic M Series oils are particularly resistant to sludge formation as a result of prolonged high temperature exposure and perform very well in turbine circulating systems - even those with short oil residence times. This combination of benefits makes Teresstic M Series the right choice for MHI turbine users.

The Teresstic M Series of products are designed to provide a reliable lubricant solution for MHI and GE non-geared gas and steam turbines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 9595Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 32 cSt32 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 5.09 cSt5.09 cStASTM D445
Oxidative Stability 500 hour500 hourRotating Pressure Vessel Oxidation Test (RPVOT); ASTM D2272
 
Thermal PropertiesMetricEnglishComments
Pour Point -12.0 °C10.4 °FASTM D97
Flash Point 200 °C392 °FASTM D92
 
Descriptive Properties
Air Release, ASTM D3427, minutes4 (max)@ 50°C
Demulsibility Time (min)15 (max)to 3 mL emulsion @ 54°C
Foam Sequence I, ASTM D97950/0
Foam Sequence II, ASTM D89350/0
Foam Sequence III, ASTM D89350/0
Neutralization Number, ASTM D9740.2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WEXXON159 / 75584

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.