MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubrizol Estane® ALR CL60D Thermoplastic Polyurethane  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Type: Estane® ALR CL600 is a Shore D thermoplastic polyurethane (TPU) resin.

Features: Contains a UV package that enhances outdoor weatherability, but does not contain lubricants or wax processing aids.

Uses: Outdoor applications

Information Provided by The Lubrizol Corporation

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccASTM D792
Melt Flow 3.2 g/10 min
@Load 2.16 kg,
Temperature 175 °C
ASTM D1230
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 57ASTM D2240
Tensile Strength, Ultimate 9350 psiASTM D412
Tensile Strength, Yield 2185 psiat 100%; ASTM D412
 3765 psiat 200%; ASTM D412
Elongation at Break 370 %ASTM D412
Flexural Modulus 9200 psiASTM D790
 
Processing PropertiesOriginal ValueComments
Feed Temperature 175 °C
Middle Barrel Temperature 180 °C
Nozzle Temperature 185 °C
Melt Temperature 185 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol Estane® ALR CL57D Thermoplastic Polyurethane
Lubrizol Estane® AG 9550 Thermoplastic Polyurethane
Lubrizol Estane® ALR CL87A Thermoplastic Polyurethane
Lubrizol Estane® ALR CL65D Thermoplastic Polyurethane
Lubrizol Estane® ALR E68D-V Thermoplastic Polyurethane

PNOVEON568 / 121459

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.