MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Teijin Films Mylar® DS Polyester Film
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Mylar® DS is a super clear, biaxially oriented, polyester film with differential surface roughness on each side. Its unique composition, consisting of a smooth side opposite a rougher, filled side, allows for a high clarity product with superior handling characteristics. Mylar® DS is suitable for a broad range of applications including high-speed metallization, lamination, and coating. Mylar® DS1 is 1-side treated on the smooth side for adhesion promoting. Mylar® DS1A is 1-side treated on the rough side for adhesion promoting. Mylar® DS2 is treated on both sides for adhesion promoting.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.39 g/ccTypical Mylar®; ASTM D1505
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 140 %ASTM D882A
Film Elongation at Break, TD 100 %ASTM D882A
Coefficient of Friction, Static 0.40A-B; ASTM D1894
Film Tensile Strength at Break, MD 28000 psiASTM D882A
Film Tensile Strength at Break, TD 32000 psiASTM D882A
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.17 J/g-°CTypical Mylar®
Melting Point 254 °CTypical Mylar® via DSC
Shrinkage, MD 3.0 %
@Temperature 190 °C,
Time 300 sec
Unrestrained
Shrinkage, TD 1.0 %
@Temperature 190 °C,
Time 300 sec
Unrestrained
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.64 - 1.67typical of Mylar®
Haze 1.0 %
@Thickness 0.0234 mm
ASTM D1003
 1.2 %
@Thickness 0.0361 mm
ASTM D1003
 1.4 %
@Thickness 0.0508 mm
ASTM D1003
 
Descriptive Properties
Yield (nominal)13970 in2/lb142 Gauge
 21800 in2/lb92 Gauge
 9900 in2/lb200 Gauge

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® D804 Polyester Film, 60 Gauge
DuPont Teijin Films Mylar® EB31 Polyester Film, 92 Gauge
DuPont Teijin Films Mylar® EB11 Polyester Film, 48 Gauge
DuPont Teijin Films Mylar® A Polyester Film, 48 Gauge
DuPont Teijin Films Mylar® ADS Polyester Film, 200 Gauge

PDTZ9300 / 139622

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.