MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Ineos Nova 1301 High Heat Crystal Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Heat Resistant Grade

Material Notes: High heat resistance, High strength, Good processing characteristics, USP Class VI

Applications: Electronics packaging, Medical packaging, Cosmetic cases, Profile extrusion

Exposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and optical properties of the material.

Properties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.

Information provided by NOVA Chemicals.

INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. 

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmASTM D955
Melt Flow 3.5 g/10 minCondition G
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 75
Tensile Strength, Yield 48.0 MPaASTM D638
Elongation at Break 2.0 %ASTM D638
Flexural Yield Strength 76.0 MPaASTM D790
Flexural Modulus 3.037 GPaASTM D790
Izod Impact, Notched 0.200 J/cm
@Diameter 3.17 mm
bar, 0.010" notch radius; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.59
@Frequency 1e+6 Hz
Dielectric Strength 500 kV/in
@Thickness 3.17 mm
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °CASTM D648
Vicat Softening Point 106 °CASTM D1525
Flammability, UL94 HB
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.59
@Wavelength 589.3 nm
sodium D line
Optical Density 0.046400-700 mm avg.
Transmission, Visible 88 - 90 %at 550 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 190 - 274 °C
Mold Temperature 38.0 - 82.0 °C
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos Nova 1300 High Heat Crystal Polystyrene
Americas Styrenics STYRON® 666D High Heat Crystal Polystyrene
Celanese Zytel® 101L NC010 PA66
Ineos Nova 1204 High Heat Crystal Polystyrene
Ineos Nova 1504 High Heat Crystal Polystyrene

PNOVA008 / 54909

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.