MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Exceed™ 3518 CB Premium Cast Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Hexene, Film Grade

Material Notes: Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. These superior properties, along with excellent drawability, make these resins versatile for both monolayer and multilayer cast packaging film.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Processing Aid: No
  • Thermal Stabilizer: Yes
Applications:
  • Bag in Box
  • Barrier Food Packaging
  • Blown Film
  • Cast Film
  • Cast Stretch Film
  • Diaper Backsheet
  • Food Packaging
  • Form Fill and Seal Packaging
  • Hygiene Film
  • Packaging Fims
  • Personal Care
Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccExxonMobil Method
Thickness 0.800 mil
Melt Flow 3.5 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 1200 psiat 2% offset; ASTM D882
Film Tensile Strength at Yield, TD 1100 psiat 2% offset; ASTM D882
Film Elongation at Break, MD 510 %ASTM D882
Film Elongation at Break, TD 680 %ASTM D882
Puncture Energy 3.17 ft-lbExxon Mobil Method
Elmendorf Tear Strength MD 190 gASTM D1922
Elmendorf Tear Strength TD 500 gASTM D1922
Elmendorf Tear Strength, MD 237.5 g/milASTM D1922
Elmendorf Tear Strength, TD 625 g/milASTM D1922
Dart Drop 175 g/milASTM D1709
Dart Drop Test 140 gASTM D1709
Film Tensile Strength at Break, MD 10700 psiASTM D882
Film Tensile Strength at Break, TD 6770 psiASTM D882
1% Secant Modulus, MD 16000 psiASTM D882
1% Secant Modulus, TD 18000 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 237 °FPeak Melting Temperature; ExxonMobil Method
 
Optical PropertiesOriginal ValueComments
Haze 2.4 %ASTM D1003
Gloss 86 %45°; ASTM D2457
 
Descriptive Properties
FeaturesThermal Stabilizer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Exceed™ m 3518.PA Cast Premium Cast Film Resin
Dow ELITE™ 5230G Enhanced Polyethylene Resin
Chevron Phillips Marlex® 1412 Injection Molding Resin
ExxonMobil Enable™ 27-03HH Metallocene Polyethylene Resin (European Grade)
ExxonMobil Exceed™ 1018KA Metallocene Polyethylene Resin (Asia Pacific Grade)

PEXB127 / 37432

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.