MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Teijin Films Teijin® Tetoron® HB3 Polyester Film, 200 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Teijin® Tetoron® HB3 is a super smooth polyester film with a UV absorbing agent, originally designed for green house applications. It has excellent weather-durability, low color and low haze. It is pretreated on one side for slip and is available plain or knurled.

Typical Applications:

  • Greenhouse film
  • Open air Labels
  • Solar Window Film

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 2.00 mil
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 160 %ASTM D882A
Film Elongation at Break, TD 120 %ASTM D882A
Coefficient of Friction, Dynamic 0.32ASTM D1894
Coefficient of Friction, Static 0.31ASTM D1894
Film Tensile Strength at Break, MD 32625 psiASTM D882A
Film Tensile Strength at Break, TD 35525 psiASTM D882A
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD 1.0 %
@Temperature 150 °C,
Time 1800 sec
Unrestrained
Shrinkage, TD 0.20 %
@Temperature 150 °C,
Time 1800 sec
Unrestrained
 
Optical PropertiesOriginal ValueComments
Haze 0.40 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Teijin Films Teijin® Tetoron® HSL Polyester Film, 300 Gauge
DuPont Teijin Films Teijin® Tetoron® HS Polyester Film, 300 Gauge
DuPont Teijin Films Mylar® XG2 Polyester Film, 92 Gauge
DuPont Teijin Films Teijin® Tetoron® G2 Polyester Film, 65 Gauge
DuPont Teijin Films Teijin® Tetoron® O Polyester Film, 300 Gauge

PDTZ9451 / 139768

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.