MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemical Concepts Chem-Set™ RTV4500 Acetoxy cure silicone sealant
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: Chem-Set™ RTV 4500 is a one component room temperature vulcanizing (RTV) industrial/construction grade silicone sealant and adhesive that has been chemically formulated for high strength adhesion. When fully cured, this unique VOC compliant formula offers UV stability and excellent adhesion to form waterproof and airtight bonds to metal, steel, tile, fiberglass, ceramic, glass, aluminum, painted surfaces, wood, plywood, marble, plus many other common substrates.

This product is offers all weather performance to meets Green Building Standards. Features and Benefits: High Strength, Excellent Weatherability, UV Stable, Non-Yellowing, VOC Compliant, Non-Flammable, Waterproof , Excellent Adhesion, Non-Shrinking, Construction & Industrial Applications: Kitchen And Bath, Countertops/Backsplashes, Sealing & Glazing, HVAC/R , Plumbing, Roofing, Sanitary Seals, Precast Concrete, Transportation Seals, Marine Cabins, Appliance Trim, Interior/Exterior, Above Grade.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/cc
@Temperature 25.0 °C
50% RH
Volatile Organic Compounds (VOC) Content 30 g/l
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 26Tested at 77°F & 50% RH; ASTM C661
Tensile Strength 310 psiTested at 77°F & 50% RH; ASTM D412
Elongation at Break 500 %Tested at 77°F & 50% RH; ASTM D412
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.7
@Frequency 100 Hz
Tested at 77°F & 50% RH
Dielectric Strength 500 V/milTested at 77°F & 50% RH
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 350 °F
 400 °Fintermittent
Minimum Service Temperature, Air -62.0 °F
 
Processing PropertiesOriginal ValueComments
Extrusion Rate >= 370 g/min1/8" orifice @ 50 psi, modified.; ASTM C 1183
Shelf Life 24.0 MonthTested at 77°F & 50% RH
 
Descriptive Properties
AppearanceRubber, cured
Colorclear, white, black, aluminum, almond, bronze, gray, trans white, custom colors available. Tested at 77°F & 50% RH

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHEMI961 / 232178

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.