MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil HD 5403 Blow Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Product Description: ExxonMobil™ HD 5403 is a high density polyethylene blow molding grade offering a good combination of stiffness and stress crack resistance.

Availability: Africa & Middle East; Europe, Latin America, North America

Additive:

  • Thermal Stabilizer: Yes
  • Antistatic: No
Applications:
  • Drainage Pipes
  • Food packaging
  • Household and Industrial chemical containers
  • Pharmaceutical Packaging
  • Thermoformed Parts
  • Thin Gauge Sheet
Information provided by ExxonMobil Chemical

Key Words: Paxon™ AL55-003
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.954 g/ccASTM D4883
ESCR 100% Igepal® 30 hourASTM D1693 Condition B
Melt Flow 0.30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 63.0
@Time 15.0 sec
ASTM D2240
Tensile Strength at Break 29.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 4100 psiASTM D638
Elongation at Yield 9.00 %ASTM D638
Flexural Modulus 130000 psi2% Secant; ASTM D790
Flexural Modulus, 1% Secant 1.10 GPaASTM D790A
Charpy Impact, Notched 0.600 J/cm²
@Temperature -20.0 °C
ISO 179/1eA
 1.00 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Crystallization Temperature 118 °C
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °CASTM D648
Vicat Softening Point 260 °FASTM D1525
Brittleness Temperature <= -105 °FASTM D746
 
Processing PropertiesOriginal ValueComments
Melt Temperature 268 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Alathon® L5440 High Density Polyethylene
Dow UNIVAL™ DMDA-6200 NT 7 High Density Polyethylene Resin (HDPE)
ExxonMobil Paxon™ AM55-003 Blow Molding Resin
ExxonMobil Paxon™ AG45-004 Blow Molding Resin
ExxonMobil Paxon™ 7204 Crosslinkable Rotational Molding Resin

PEXB098 / 37403

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.