MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Polymer Resources PEI-G30 Polyetherimide, 30% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyetherimide (PEI); Polyetherimide (PEI), 30% Glass Fiber

Material Notes: Polyetherimide, 30% Glass Reinforced

Process: Injection Molding
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.

Information provided by Polymer Resources Corporation.

Key Words: UL E113219
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.51 g/cc1.51 g/ccASTM D792
Water Absorption 0.16 %
@Time 86400 sec
0.16 %
@Time 24.0 hour
ASTM D570
Moisture Absorption at Equilibrium 0.90 %0.90 %ASTM D570
Linear Mold Shrinkage 0.0010 - 0.0040 cm/cm0.0010 - 0.0040 in/inASTM D955
Melt Flow 5.0 - 22 g/10 min
@Load 6.70 kg,
Temperature 337 °C
5.0 - 22 g/10 min
@Load 14.8 lb,
Temperature 639 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 114114ASTM D785
Tensile Strength at Break 162 MPa23500 psiASTM D638
Tensile Strength, Yield 162 MPa23500 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Tensile Modulus 9.31 GPa1350 ksiASTM D638
Flexural Strength 221 MPa32000 psiASTM D790
Flexural Modulus 8.27 GPa1200 ksiASTM D790
Izod Impact, Notched 0.801 J/cm
@Temperature 22.8 °C
1.50 ft-lb/in
@Temperature 73.0 °F
ASTM D256
Izod Impact, Unnotched 4.27 J/cm
@Temperature 22.8 °C
8.00 ft-lb/in
@Temperature 73.0 °F
ASTM D4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.00e+16 ohm-cm3.00e+16 ohm-cmASTM D257
Dielectric Constant 3.7
@Frequency 1000 Hz
3.7
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 24.4 kV/mm620 kV/inin air; ASTM D149
 29.9 kV/mm760 kV/inin oil; ASTM D149
Dissipation Factor  0.0015
@Frequency 1000 Hz
0.0015
@Frequency 1000 Hz
ASTM D150
 0.0053
@Frequency 1e+9 Hz
0.0053
@Frequency 1e+9 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 18.0 µm/m-°C
@Temperature -20.0 - 150 °C
10.0 µin/in-°F
@Temperature -4.00 - 302 °F
ASTM E831
CTE, linear, Transverse to Flow 41.4 µm/m-°C
@Temperature -20.0 - 150 °C
23.0 µin/in-°F
@Temperature -4.00 - 302 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 211 °C412 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FASTM D648
Vicat Softening Point 227 °C440 °F120°C/h, 50 N; ASTM D1525
UL RTI, Electrical  105 °C
@Thickness 1.50 mm
221 °F
@Thickness 0.0591 in
UL 746
 105 °C
@Thickness 3.00 mm
221 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact  105 °C
@Thickness 1.50 mm
221 °F
@Thickness 0.0591 in
UL 746
 105 °C
@Thickness 3.00 mm
221 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact  105 °C
@Thickness 1.50 mm
221 °F
@Thickness 0.0591 in
UL 746
 105 °C
@Thickness 3.00 mm
221 °F
@Thickness 0.118 in
UL 746
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 332 - 399 °C630 - 750 °F
Middle Barrel Temperature 338 - 399 °C640 - 750 °F
Front Barrel Temperature 343 - 399 °C650 - 750 °F
Melt Temperature 338 - 399 °C640 - 750 °F
Mold Temperature 107 - 177 °C225 - 350 °F
Drying Temperature 143 - 149 °C290 - 300 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Vent Depth 0.00254 cm0.00100 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Oxford Polymers 20GF 20% Glass Fiber Filled Polyetherimide for Extrusion and Injection Molding
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 900
LATI Larpeek 50 G/30 PEEK, 30% Glass Fiber Reinforced
Oxford Polymers 30GF 30% Glass Fiber Filled Polyetherimide for Extrusion and Injection Molding
Ensinger TECAPEI® 30% Glass Reinforced, made from Ultem® 2300 PEI

PPOLYQ197 / 160718

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.