MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Agility™ 1002 Performance LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: Product Description: Agility 1002 Performance LDPE is a high pressure LDPE resin designed specifically to run at faster output rates on blown film lines in blends with LLDPE resins while maintaining bubble stability. This resin includes 2,000 ppm of anti-block to minimize blocking issues.
Main Characteristics:
  • Faster processing LDPE resin
  • Designed for higher output rates in blends with LLDPE resins at 10-20% loading
  • Optimized molecular structure gives improved optics in blends with LLDPE resins
Complies with: US FDA 21 CFR 177.1520 ©2.2; EU No 10/2011; Canadian HPFB No Objection. Consult the regulations for complete details.

Availability: Europe; North America

Additive: Antiblock: 2000 ppm; Processing Aid: No; Slip: No

Agency Ratings: FDA 21 CFR 177.1520 ©2.2; EU No 10/2011; Canadian HPFB No Objection

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.922 g/cc0.0333 lb/in³ASTM D792
Melt Flow 0.65 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.65 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Puncture Resistance 22.2 N5.00 lb (f)
Film Tensile Strength at Yield, MD 28.3 MPa4100 psiASTM D882
Film Tensile Strength at Yield, TD 13.0 MPa1880 psiASTM D882
Film Elongation at Break, MD 110 %110 %ASTM D882
Film Elongation at Break, TD 430 %430 %ASTM D882
1% Secant Modulus 243 MPa35300 psiMD; ASTM D882
 301 MPa43600 psiTD; ASTM D882
2% Secant Modulus 0.221 GPa32.1 ksiMD; ASTM D882
 0.255 GPa37.0 ksiTD; ASTM D882
Puncture Energy 0.565 J0.417 ft-lb
Elmendorf Tear Strength MD 290 g290 gASTM D1922
Elmendorf Tear Strength TD 95 g95 gASTM D1922
Dart Drop Test 75.0 g0.165 lbASTM D1709A
Film Tensile Strength at Break, MD 29.6 MPa4300 psiASTM D882
Film Tensile Strength at Break, TD 16.2 MPa2350 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 109 °C228 °F
Vicat Softening Point 93.9 °C201 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 10 %10 %ASTM D1003
Gloss 51 %51 %45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 203 °C398 °FExtrusion
Blow-up Ratio (BUR) 2.52.5
 
Descriptive Properties
Film Puncture Resistance30 ft-lb/in3
Film Toughness320 ft-lb/in3MD, ASTM D882
 620 ft-lb/in3TD, ASTM D882

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF385 / 311078

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.