MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
ITW Permatex® The Right Stuff®
Categories: Polymer; Adhesive; Thermoset

Material Notes: PERMATEX® The Right Stuff? is a single component, room temperature curing, elastomeric gasketing compound designed to provide reliable “formed-in-place” gaskets for mechanical assemblies. The Right Stuff® is a non-slumping, non-corrosive, low odor, low volatile, single component, proprietary, hi-tech, elastomeric rubber gasketing material. It has been designed specifically as a replacement for conventional cut gaskets where instant sealability is advantageous. The product resists aging, weathering and thermal cycling without hardening, shrinking or cracking. Designed for superior bonding properties to oil contaminated metals as compared to other formed-in-place gaskets, and maintains outstanding oil resistance. NSF White Book registered.

The surface of this adhesive becomes dry to touch on exposure to atmospheric moisture within 15 minutes at 23± 2°C, 50 ± 5% RH. The product cures on exposure to moisture in the air and dries tack free in two hours, with full cure in 24 hours. Cure times will vary with temperature, humidity and gap.

It retains effective properties in contact with automotive fluids, such as motor oil, transmission fluids, alcohol and antifreeze solutions. Note: Not recommended for parts in contact with gasoline.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 g/ccUncured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 25 - 35ASTM D2240
Tensile Strength 203.1 psiASTM D412
Elongation at Break 550 %ASTM D412
Adhesive Bond Strength 150 psiAluminum (T2024) After 21 days @ 23°C, 50% RH at 0.5 mm gap. Isopropanol wiped substrate; ASTM D1002
 150 psiMild Steel. After 21 days @ 23C, 50% RH at 0.5 mm gap. Isopropyl Alcohol wiped substrates; ASTM D1002
 180 psiZinc Dichromate After 21 days @ 23°C, 50% RH at 0.5 mm gap. Isopropanol wiped substrate; ASTM D1002
 180 psiAluminum (Alclad) After 21 days @ 23°C, 50% RH at 0.5 mm gap. Isopropanol wiped substrate; ASTM D1002
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 200 °F
 
Descriptive Properties
Chemical TypeElastomeric Rubber
ColorMetallic BlackUncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWP9146 / 239656

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.