MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
P & P Technology EPDM Closed Cell Sponge
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: Metweave is a lamination of PPT conductive fabric and closed cell EPDM.

Information provided by P & P Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.110 - 0.150 g/cc
Water Absorption <= 0.80 %Vacuum
Deformation 25 %
@Pressure 0.0200 - 0.0400 MPa
Compression
 50 %
@Pressure 0.0700 - 0.100 MPa
Compression
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 35 - 55
Tensile Strength 0.220 MPa
Elongation at Break >= 180 %
Tear Strength >= 1.00 kN/m
Compression Set <= 30 %
@Temperature 23.0 °C,
Time 79200 sec
0.5
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 120 °C
Minimum Service Temperature, Air -40.0 °C
Flammability, UL94 V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polykemi AB POLYelast TPE EC88R Thermoplastic Elastomer, PP/EPDM
NASCA Elastomers Fulxus® FX-TPV190 Olefinic Elastomer
Polykemi AB POLYelast TPE E606 Thermoplastic Elastomer, EPDM-based
Polykemi AB POLYelast TPE E706 Thermoplastic Elastomer, EPDM-based
3M SJ-4FB Cold Shrink Foldback Splice Jacket Kits

PPPTEC015 / 133479

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.