MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Saint-Gobain Tygon® Noroprene® Chemical Tubing Formulation  (discontinued **)
Categories: Polymer; Thermoplastic

Material Notes: Norprene® Chemical Tubing is a high performance co-extruded product specifically formulated to provide an ideal combination of chemical resistance and pump life. Its inert ultra-smooth plasticizer-free bore resists the absorption/adsorption of aqueous fluids while the Norprene® outer jacket provides long flex life in peristaltic pumps. Norprene® Chemical Tubing is an excellent choice for sensitive fluid transfer applications.

Outstanding Chemical Life

The inner liner of Norprene® Chemical Tubing significantly increases the chemical resistance and allows for a broader range of usability. The tubing is virtually unaffected by acids, bases, salts, ketones and alcohols allowing its use in a wide range of chemical applications without the use of multiple tubings.

Superior Pump Life

The outer jacket of Norprene® Chemical Tubing is extremely flexible, expanding the pump life of the tubing and reducing downtime due to pump tubing failure.

Features and Benefits

  • Long flex life in peristaltic pumps
  • Temperature range of -75° F to 165° F
  • Superior chemical resistance
  • Plasticizer-free bore
  • Meets FDA criteria for food contact
  • Resists absorption adsorption of aqueous fluids
  • Virtually unaffected by chemical sanitizers and cleaners
  • Complies with FDA 21 CFR, 177.1520 criteria and is applicable for food contact applications
  • Unaffected by most commercial sanitizers and cleaners
  • Can be autoclaved for up to five cycle times without affecting its overall service life

Regulatory Information: This product complies with FDA and NSF 51 criteria.

Unless otherwise noted, all tests were conducted at room temperature. Values shown were determined on 1.9 mm thick extruded strip or 1.9 mm thick molded ASTM placques or molded ASTM durometer buttons.

Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.980 g/ccASTM D792
Water Absorption <= 0.010 %
@Temperature 22.8 °C,
Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 61
@Time 15.0 sec
ASTM D2240
Tensile Strength 1000 psiASTM D412
Elongation at Break 375 %ASTM D412
Tear Strength 120 pliASTM D1004
Compression Set 30 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395 Method B
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 165 °F
Brittleness Temperature -75.0 °FASTM D746
 
Compliance PropertiesOriginal ValueComments
FDA Yes
NSF Yes
 
Descriptive Properties
ColorCream

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Pharmed® Biocompatible Tubing for Peristaltic Pumps and Cell Culture
Saint-Gobain Tygon® A-60-G Industrial Grade Tubing Formulation
Saint-Gobain Tygon® A-60-F Food Process Tubing Formulation
Saint-Gobain Tygon® S3™ E-LFL Long-Flex Life Pump Tubing Formulation
Saint-Gobain Tygon® A-60-F I.B. Pressure Tubing Formulation for CIP and SIP cleaning and sterilization systems

PSTGQ910 / 160406

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.