MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Chemlon® 100 Nylon 66, Unreinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced, Flame Retardant

Material Notes: Features: Basic nylon 66 with internal lubrication. Widely used for automotive, electronic and appliance applications.

Processing Method: Injection Molding

Forms: Pellets

Automotive Specifications: Ford ESB-M4D150-A; Ford ESF-M4D150-A

Information Provided by Teknor Apex

Key Words: Polyamide 66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.14 g/ccASTM D792
Water Absorption 1.2 %24 hr; ASTM D750
Linear Mold Shrinkage 0.015 - 0.022 in/inASTM D955
Melt Flow 10 g/10 min
@Load 0.325 kg,
Temperature 235 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 12500 psiASTM D638
Elongation at Break 50 %ASTM D638
Elongation at Yield 5.0 %ASTM D638
Flexural Strength 16000 psiASTM D790
Flexural Modulus 415000 psiASTM D790
Izod Impact, Notched 1.10 ft-lb/in
@Temperature 22.8 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+18 ohm-cmASTM D257
Dielectric Strength 460 V/mil
@Thickness 3.00 mm
ASTM D149
Comparative Tracking Index 600 VUL 746
 
Thermal PropertiesOriginal ValueComments
CTE, linear 39.0 µin/in-°FASTM D696
Melting Point 495 °FDSC
Deflection Temperature at 0.46 MPa (66 psi) 428 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 195 °FUnannealed; ASTM D648
UL RTI, Electrical 239 °F
@Thickness 0.810 mm
UL 746
 239 °F
@Thickness 1.50 mm
UL 746
 239 °F
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical with Impact 167 °F
@Thickness 0.810 mm
UL 746
 167 °F
@Thickness 1.50 mm
UL 746
 185 °F
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical without Impact 203 °F
@Thickness 0.810 mm
UL 746
 203 °F
@Thickness 1.50 mm
UL 746
 203 °F
@Thickness 3.00 mm
UL 746
Flammability, UL94 V-2
Oxygen Index 27 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 465 - 490 °F
Middle Barrel Temperature 495 - 525 °F
Front Barrel Temperature 505 - 540 °F
Nozzle Temperature 505 - 535 °F
Melt Temperature 505 - 535 °FProcessing Temperature
Drying Temperature 175 °F
Moisture Content 0.20 %
 
Descriptive Properties
Suggested Regrind, max25

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Chemlon® 109 Nylon 66, Impact Grade
Teknor Apex Chemlon® 100 W Nylon 66, Unreinforced
Celanese Zytel® 101 NC010 PA66
ExxonMobil Santoprene® 101-64 Thermoplastic Elastomer
Firestone CL200-001 Nylon 6

PTEKNO425 / 128602

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.