MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ferro Aluminum Oxide P99
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Manufactured at the Diamonite Plant in Shreve, Ohio. Data provided by the manufacturer, Ferro Corporation.

Key Words: Al2O3, alumina, aluminium oxide, aluminum oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.90 - 3.94 g/cc
Water Absorption 0.00 %
Open Porosity 0.00 %Gas tight. Test with helium mass spectrometer
Weibull Modulus 10
 
Mechanical PropertiesOriginal ValueComments
Knoop Microhardness 1400KHN5 microhardness, kg/mm²
Vickers Microhardness 1530HV5 microhardness, kg/mm²
Tensile Strength, Ultimate 215 MPaACMA Test #4
Modulus of Elasticity 331 GPaultrasonic
Compressive Strength 1800 MPaASTM C773-74
Poissons Ratio 0.26ASTM C623
Fracture Toughness 4.30 MPa-m½Kic (indentation)
Shear Modulus 131 GPaultrasonic
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.60e+7 ohm-cm
@Temperature 700 °C
ASTM D257
 5.50e+8 ohm-cm
@Temperature 500 °C
ASTM D257
 2.50e+11 ohm-cm
@Temperature 300 °C
ASTM D257
 1.50e+15 ohm-cm
@Temperature 100 °C
ASTM D257
Dielectric Constant 9.8
@Frequency 1e+6 Hz
ASTM D-116
Dielectric Strength 8.46 kV/mm
@Thickness 6.35 mm
ASTM D149
Dissipation Factor 0.0020
@Frequency 1e+6 Hz
ASTM D-116
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.10 µm/m-°C
@Temperature 25.0 - 200 °C
ASTM C32
 7.40 µm/m-°C
@Temperature 25.0 - 500 °C
ASTM C32
 8.10 µm/m-°C
@Temperature 25.0 - 800 °C
 8.50 µm/m-°C
@Temperature 25.0 - 1000 °C
ASTM C32
Thermal Conductivity 35.4 W/m-K
 5.40 W/m-K
@Temperature 1000 °C
 6.30 W/m-K
@Temperature 800 °C
 10.1 W/m-K
@Temperature 400 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 99.5 %
 
Descriptive Properties
ColorOff White

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
GBC Grade 99 Alumina
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3
Anderman Ceramics EA99P Sintered Alumina, 99%, Porous
CeramTec B 40 Alumina, 99.1%
Goodfellow Shapal™-M soft Aluminum Nitride (AlN) - Machinable

CFC012 / 810

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.