MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ITW Devcon® Wear Guard™ Ultra Wear-Resistant Epoxy Compound
Categories: Polymer; Thermoset; Epoxy

Material Notes: Alumina ceramic bead-filled epoxy system with outstanding abrasion resistance for severe service conditions. Use; Repair scrubbers, ash handling systems, pipe elbows, screens and ceramic lined chutes; recontour chippers, bins, hoppers, bunkers, separators; protect exhausters, chutes, launders, housing fans, crushers and breakers. Features: Extends Equipment Operating Cycles, Epoxy Primer FC included (For use as primer), Non-sagging, Outstanding Wear Resistance.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.50 g/ccCured
Solids Content 100 %Uncured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 87
Tensile Strength 4260 psi
Flexural Strength 8735 psi
Compressive Strength 13910 psi
Adhesive Bond Strength 1565 psiLap Shear; w/o beads
Taber Abrasion, mg/1000 Cycles 0.065Weight loss (grams). w/o beads
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 16.0 hourFunctional cure
Pot Life 20.0 min
@Temperature 23.9 °C
 
Descriptive Properties
Chemical/Solvent ResistanceSodium Hydroxide 10%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Sulfuric Acid 10%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
ColorGrayuncured
Coverage44 sq.in/lbCured @ 1/4"
Mix Ratio by weightR:18.8/H:7.8/Beads:73.4
Recoat Time1 to 2 hrs
ViscosityNon-sag putty Mixed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWD9176 / 239686

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.