MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro DUREFLEX® X2103 TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Characterization: Dureflex X2103 is an aromatic polyether polyurethane film/sheeting product specially formulated with a non-halogenated fire retardant.

Properties / Applications: Dureflex X2103, as a polyether TPU, it exhibits excellent hydrolysis and fungus resistance, and therefore is recommended for applications that have continuous exposure to water and high humidity environments. This product is recommended for adhesion to fabrics as a protective and adhesive layer, or as a “stand alone ” film in demanding applications that require flame retardancy. If your application will experience continuous exposure to petrochemicals such as gasoline, diesel fuel, aviation fuel, and many solvents, consider using Dureflex brand polyester polyurethane film and sheet grades. As with any product, use of Dureflex X2103 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.23 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 88ASTM D2240
Tensile Strength, Ultimate 5000 psiMD/CD Ave; ASTM D882
Elongation at Yield 500 %Ultimate; ASTM D882
100% Modulus 0.00758 GPa
@Strain 100 %
MD/CD Ave; ASTM D882
300% Modulus 0.0152 GPa
@Strain 300 %
MD/CD Ave; ASTM D882
Tear Strength 400 pliMD/CD Ave; ASTM D1004
 
Thermal PropertiesOriginal ValueComments
Softening Point 149 - 168 °CASTM E2347-004

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro DUREFLEX® PS5400 TPU
Covestro DUREFLEX® U073 TPU
Covestro DUREFLEX® PT6400 TPU
Covestro DUREFLEX® PS8400 TPU
Covestro DUREFLEX® U04 TPU

PCOVEST0775 / 202558

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.