MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Phon Tech PHOENIX™ 02501 Translucent TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Utilizing the characteristics of SBC Copolymers Compounds (SEBS Compounds, SEPS Compounds), PHOENIX™ Translucent Thermoplastic Elastomers (TPEs) demonstrate powerful physical properties in elongation, tensile strength, tear strength and compression set. This SEBS based TPE compound family is originated for components which mechanical properties are critical points. Moreover, the hardness, touch feel and finish can be customized to widen the variety of products and give the desired effects. No matter what you request, matt finish, slippery feels, shiny appearance, silky smooth or more, PHOENIX™ Translucent Thermoplastic Elastomers (TPEs) are versatile material for you.

Features:

  • Wide range hardness (Shore 15A ~ 65D)
  • Anti-slip
  • Anti-scratch
  • Non-sticky
  • Easy to process and color
  • Excellent elongation and elasticity
  • Excellent tensile strength
  • Excellent weather resistance and heat resistance (up to 100?)
  • Very good resilience
  • Meet FDA requirements
Applications: Medical tube, hand tools grip, syringe stopper, medical caster wheel, cable and wire sheath, film, sheet, extrusion profiles, etc.

Information provided by Phon Tech Industrial Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.850 - 0.910 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 47 - 53ASTM D2240
Tensile Strength 791.4 psiASTM D412
Elongation at Break 901.2 %ASTM D412
100% Modulus 187.7 psiASTM D412
Tear Strength 112 pliASTM D624 Die C
 
Descriptive Properties
ColorTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPHONT012 / 296354

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.