MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
INEOS Styrolution Polystyrol 168 N GR 2 PS
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Molded, Unreinforced

Material Notes: Styrolution PS 168N is a high molecular weight, heat resistant grade used where high strength is required. Suitable for physically or chemically expanded extruded sheet. Also use as a blend component with high impact polystyrene or Styrolux SBC. High molecular weight, heat resistant grade used where high, strength is required. Suitable for physically or chemically expanded extruded sheet, Suitable for physically or chemically expanded extruded sheet, Blend with high impact polystyrene or Styrolux SBC. Applications: Foamed meat trays, foamed labels., In mixtures with high impact polystyrene for coffee cups, lids, etc., In mixtures with Styrolux for transparent, impact resistant cups,, beakers and lids.

Information provided by STYROLUTION, which is a joint venture between BASF and INEOS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.600 g/ccwith external lubricant
Density 1.048 g/ccISO 1183
Moisture Absorption at Equilibrium <= 0.10 %
@Temperature 23.0 °C
50% RH; ISO 62
Water Absorption at Saturation <= 0.10 %
@Temperature 23.0 °C
ISO 62
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cmISO 294-4
Melt Flow 1.2 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ISO 1133
 1.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 150 MPaISO 2039-1
Tensile Strength, Yield 59.0 MPaISO 527
Elongation at Break 3.0 %ISO 527
Tensile Modulus 3300 MPaISO 527
Flexural Strength 106 MPaISO 178
Izod Impact, Notched (ISO) 2.00 kJ/m²
@Temperature 23.0 °C
ISO 180/A
 2.00 kJ/m²
@Temperature -30.0 °C
ISO 180/A
Charpy Impact Unnotched <= 25.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 4.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
Tensile Creep Modulus, 1 hour 3300 MPaISO 899
Tensile Creep Modulus, 1000 hours 2600 MPaISO 899
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+18 ohm-cmIEC 60093
Surface Resistance >= 1.00e+14 ohmIEC 60093
Dielectric Constant 2.5
@Frequency 100 Hz
IEC 60250
 2.5
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 135 kV/mmShort time, 1.5 mm; IEC 60243-1
Dissipation Factor 0.000050
@Frequency 1e+6 Hz
IEC 60250
 0.000090
@Frequency 100 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°CISO 11359
Thermal Conductivity 0.170 W/m-KDIN 52612-1
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °Cannealed 4 hours at 80°C; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °Cannealed 4 hours at 80°C; ISO 75
Vicat Softening Point 101 °C
@Load 5.10 kg
VST/B/50. 50C/h; ISO 306
 108 °C
@Load 1.02 kg
B/1 120C/h; ASTM D 1525
 
Processing PropertiesOriginal ValueComments
Melt Temperature 180 - 280 °CISO 294
Mold Temperature 10.0 - 60.0 °CISO 294
Injection Velocity 200 mm/secISO 294
 
Descriptive Properties
ColorCrystal Clear 00013
Commercial StatusEurope
Primary Processing TechniqueInjection Molding and Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
INEOS Styrolution Polystyrol 143 E GR 2 PS
BASF Polystyrol® 143 E Polystyrene (Europe)
Chi Mei Polyrex® PH-88 Polystyrene - High Impact
INEOS Styrolution Polystyrol 168 N GR 21 PS
INEOS Styrolution Polystyrol 158 K GR 2 PS

PBASG0627 / 132260

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.