MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Semitron™ ESd 225 POM Extruded, Static Dissipative Acetal
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: A line of POM shapes characterized by excellent wear resistance, thermal performance, and quick dissipation of static charges. Due to these properties, this grade is ideal for several applications throughout the semiconductor and electronics industry.

Key Words: POM, Polyoxymethylene; Polyformaldehyde; Polyacetal
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.33 g/ccASTM D792
Water Absorption at Saturation 8.00 %ASTM D570 (17)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 106ASTM D785
Hardness, Shore D 75.0ISO 868
Tensile Strength 38.0 MPaISO 527-1/-2 (7)
Flexural Strength 50.0 MPaISO 178 (12)
Compressive Yield Strength 14.0 MPa
@Strain 1.00 %
ISO 604 (10)
 25.0 MPa
@Strain 2.00 %
ISO 604 (10)
 38.0 MPa
@Strain 5.00 %
ISO 604 (10)
Shear Strength 41.0 MPaASTM D732
Charpy Impact, Notched 8.00 kJ/m²ISO 179-1/1eA
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1.00e+10 - 1.00e+12 ohmANSI/ESD STM 11.11
Dielectric Constant 4.31
@Frequency 1.00e+6 Hz
ASTM D150
Dissipation Factor 0.0360
@Frequency 1.00e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 93.0 µin/in-°FASTM E-831 (TMA)
 150 µm/m-°C
@Temperature 23.0 - 100 °C
Melting Point 320 °FASTM D3418
Maximum Service Temperature, Air 190 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 225 °FASTM D648
Minimum Service Temperature, Air -50.0 °C
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Limited
Acids, Weak Limited
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Alkalies, Weak Acceptable
Chlorinated Solvents Acceptable
Continuous Sunlight Acceptable
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Unacceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Limited
 
Descriptive Properties
ESd categoryDissipative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Semitron™ ESd 490HR PEEK Non-sloughing and low moisture absorption
Mitsubishi Chemical Advanced Materials Semitron™ ESd 520HR PTFE
Mitsubishi Chemical Advanced Materials Semitron™ ESd 480 PEEK, static dissipative
Mitsubishi Chemical Advanced Materials Semitron™ ESd 420 V PEI
Mitsubishi Chemical Advanced Materials Semitron™ ESd 500 HR PTFE static dissipative, compression molded

P1SM30 / 20119

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.