MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient Elastamax™ XL 0162-19 EPDM TPV-Based Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: This is a thermoplastic elastomer based on EPDM TPV technology. This is a general purpose injection molding grade elastomer. Physical Form: Pellet. Standard Color: Opaque.

Information provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.980 g/ccASTM D792
Melt Flow 6.54 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 134 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 655 sec. delay; ASTM D2240
Tensile Strength, Ultimate 4.50 MPa10 in/min; ASTM D412
Elongation at Break 395 %10 in/min; ASTM D412
50% Modulus 0.00217 GPa
@Strain 50 %
10 in/min; ASTM D412
100% Modulus 0.00259 GPa
@Strain 100 %
ISO 37
200% Modulus 0.00325 GPa
@Strain 200 %
10 in/min; ASTM D412
300% Modulus 0.00390 GPa
@Strain 300 %
10 in/min; ASTM D412
Tear Strength 138 pliDie 'C' Tear; 20 in/min; ASTM D624
Compression Set 46 %
@Temperature 70.0 °C
22 hrs; ASTM D395
 30 %
@Temperature 23.0 °C,
Time 79200 sec
ASTM D395
Tensile Set 19 %23°C, 22 hrs.; at 100% per ASTM D412.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Elastamax™ XL 0162-26 EPDM TPV-Based Thermoplastic Elastomer
Avient Elastamax™ XL 0162-27 EPDM TPV-Based Thermoplastic Elastomer
Avient Elastamax™ XL 0162-25 EPDM TPV-Based Thermoplastic Elastomer
Avient Elastamax™ XL 0162-24 EPDM TPV-Based Thermoplastic Elastomer
Avient Elastamax™ XL 0162-21 EPDM TPV-Based Thermoplastic Elastomer

PHG220 / 46839

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.