MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Affinity™ HT 1285G Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Product Description: Affinity HT 1285G Polyolefin Plastomer (POP) is specifically designed as a high performance sealant for demanding packaging applications. It provides high packaging integrity through improved hot tack strength, enhanced caulkabilty, superior seal through contamination, and low temperature seal initiation. It helps enable hermetic packaging on today’s high speed packaging lines or with demanding substrates, and supports reducing sealant failure and potential related food waste. This product has been developed for processing on Cast, Blown, and Extrusion Coating film production liens.
  • High integrity sealant layer in flexible packaging
  • Low seal initiation temperature
  • Excellent hot tack strength
  • Excellent taste and odor profile
  • Superior seal through contamination
Complies with: EU, No 10/2011; US FDA 21 CFR 175.105; Consult the regulations for complete details

Availability: Europe; Asia Pacific; Latin America; North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: DMF; FDA FCN 424; EU No 10/2011; HPFR (Canada) No Objection; USP 23

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D792
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 841 psi
@Thickness 0.0249 mm
ASTM D882
Film Tensile Strength at Yield, TD 769 psi
@Thickness 0.0249 mm
ASTM D882
Film Elongation at Break, MD 470 %
@Thickness 0.0249 mm
ASTM D882
Film Elongation at Break, TD 720 %
@Thickness 0.0249 mm
ASTM D882
Elmendorf Tear Strength MD 78 g0.00098; ASTM D1922
Elmendorf Tear Strength TD 410 g0.00098; ASTM D1922
Dart Drop Test 290 g
@Thickness 0.0249 mm
ASTM D1709A
Film Tensile Strength at Break, MD 6960 psi
@Thickness 0.0249 mm
ASTM D882
Film Tensile Strength at Break, TD 4350 psi
@Thickness 0.0249 mm
ASTM D882
Heat Seal Strength Initiation Temperature 190 °FASTM D1525
 
Thermal PropertiesOriginal ValueComments
Melting Point 205 °F
Vicat Softening Point 178 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 4.0 %
@Thickness 0.0249 mm
Cast Film; ASTM D1003
Gloss 91 %
@Thickness 0.0249 mm
45°, Cast Film; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF376 / 311069

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.