MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Schmolz + Bickenbach Formadur® 2316/2316 ESR Plastic Mold Steel
Categories: Metal; Ferrous Metal; Tool Steel; Mold Steel

Material Notes: Increased corrosion resistance in comparison to Formadur 2083, good polishability. Usually this grade is supplied quenched and tempered to 300 HB

Applications: Molds for processing plastics with corrosive reactions

Hardening (Heat Treatment): 1020°C- 1050°C; Quenching: Oil or salt bath, 500-550°C; Hardness: 49 HRC Quenched

Information provided by Schmolz + Bickenbach

Key Words: AISI 420 Modified
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 32
@Treatment Temp. 600.0 °C
 46
@Treatment Temp. 300 °C
 46
@Treatment Temp. 400 °C
 47
@Treatment Temp. 200 °C
 47
@Treatment Temp. 500 °C
 49
@Treatment Temp. 100 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.5 µm/m-°C
@Temperature 20.0 - 100 °C
 10.7 µm/m-°C
@Temperature 20.0 - 150 °C
 10.8 µm/m-°C
@Temperature 20.0 - 200 °C
 10.9 µm/m-°C
@Temperature 20.0 - 250 °C
 11.1 µm/m-°C
@Temperature 20.0 - 300 °C
 11.3 µm/m-°C
@Temperature 20.0 - 350 °C
 11.5 µm/m-°C
@Temperature 20.0 - 400 °C
 11.6 µm/m-°C
@Temperature 20.0 - 450 °C
 11.7 µm/m-°C
@Temperature 20.0 - 500 °C
Thermal Conductivity 161 BTU-in/hr-ft²-°F
@Temperature 500 °C
 163 BTU-in/hr-ft²-°F
@Temperature 23.0 °C
 167 BTU-in/hr-ft²-°F
@Temperature 400 °C
 168 BTU-in/hr-ft²-°F
@Temperature 150 °C
 169 BTU-in/hr-ft²-°F
@Temperature 300 °C
 169 BTU-in/hr-ft²-°F
@Temperature 350 °C
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 1400 - 1472 °FSoft; Cooling: Furnace; < 230 HB
 
Descriptive Properties
Corrosion Properties/Weight loss rate0.2% Hydrochloric Acid20 g/hm2
 5% Acetic Acid0.1 g/hm2
 5% Nitric Acid1 g/hm2
 5% Sulfuric Acid90 g/hm2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Schmolz + Bickenbach Formadur® 2083 Superclean Plastic Mold Steel
Bohler-Uddeholm COMPAX™ AISI S7 MOLD QUALITY Cold Work Steel
Schmolz + Bickenbach Thermodur® 2344 EFS Extra Fine Structure - Hot Work Die Steel
300M Ultrahigh Strength Steel
AISI Grade 18Ni (250) Maraging Steel, 3.18 mm thick sheet, solution annealed at 815°C (1500°F) for 30 minutes, air cooled, aged at 455°C (850°F) for 3 hours

NSCHMO008 / 125881

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.