MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Nextel™ 550 Industrial Ceramic Fiber
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide; Other Engineering Material; Composite Fibers

Material Notes: Chemical composition above is wt%. Crystal phases are gamma alumina amorphous SiO2. Filament diameter is 10-12 µm.

3M Nextel fibers 312, 440, and 550 are designed for non-structural applications where their primary purpose is to act as a flame barrier. 3M Nextel Ceramic Fiber 550 is made from Al2O3, SiO2, and B2O3. Because 550 does not contain B2O3, this composition retains its strength better at high temperature.

Information provided by 3M Ceramic Textile and Composites.

Key Words: Alumina, Aluminum Oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.03 g/cc
Particle Size <= 0.50 µmCrystal size
Specific Surface Area <= 0.20 m²/g
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 2000 MPa
@Thickness 25.4 mm
gauge filament
Tensile Modulus 193 GPaFilament property
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.30 µm/m-°C
@Temperature 100 - 1100 °C
Melting Point 1800 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.602
 
Component Elements PropertiesOriginal ValueComments
Al2O3 73 %
SiO2 27 %
 
Descriptive Properties
ColorBlue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Nextel™ 440 Industrial Ceramic Fiber
3M Nextel™ 312 Industrial Ceramic Fiber
3M Nextel™ 610 Composite Ceramic Fiber
DuPont™ Kevlar® 149 Aramid Fiber, diam. 12 µm
3M Nextel™ 720 Composite Ceramic Fiber

CMMM02 / 1614

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.