MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Unifrax Fiberfrax® Bulk 6000 Kaolin Bulk Fiber
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Fiberfrax Bulk Fibers are manufactured to be used as feedstock in manufacturing processes or other applications where product consistency is critical. Manufactured on large, computer-controlled furnaces, these products provide customers with consistent material properties. Fiberfrax Bulk Fibers are typically used in the manufacture of other ceramic fiber based product forms such as:

  • High-temperature boards, felts, and papers
  • Combustion chambers for commercial and residential boilers
  • Riser sleeves for molten metal casting
  • Fireplace logs and panels for gas fireplaces
  • Tap out cones for molten metal applications
  • Specialized vaccum-formed shapes

These bulk fibers can also be directly used as high-temperature fill and packing material in a variety of high-temperature applications, such as:

  • Expansion joints
  • Furnace base seals
  • Tube seals
  • Burner tile packing
  • Chimney insulation

Fiberfrax 6000 Series fibers have many of the same properties as the 7000 Series fibers. The main difference is that 6000 Series fibers are manufactured from kaolin clay rather than high-purity alumina-silica raw materials. Since kaolin is a mined material, it may contain impurities such as Fe2O3, TiO2, and Na2O. Even with these impurities, Fiberfrax 6000 Series fibers can provide an effective solution in many vacuum-forming and related applications.

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.67 g/cc
 
Thermal PropertiesOriginal ValueComments
Melting Point 1760 °C
Maximum Service Temperature, Air 1175 °CRecommended Operating Temperature
 
Component Elements PropertiesOriginal ValueComments
Al2O3 45 - 51 %
Fe2O3 <= 1.5 %
NaO2 <= 0.50 %
SiO2 46 - 52 %
TiO2 <= 2.0 %
 
Descriptive Properties
Average Fiber Diameter (microns)1.5-2.5
ColorLight Gray
Fiber Index (%)45-55
Temperature Grade (°C)1260

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
6002 Aluminum Composition Spec
Magnesium AM60B-F, Die Cast
KaMin KaMin® HG90 Kaolin Clay - Ultrafine, high brightness
KaMin Hydramatte® Kaolin Clay - Filler
Imerys Kaolin Slurry™

CUNIF060 / 97832

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.