MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Microplasmic Anodizing [Ceramic Coating] for Aluminum, Magnesium, Titanium, Zirconium & Composites
Categories: Ceramic; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Microplasmic Process is for all types of aluminum, magnesium, titanium and zirconium alloys and composite materials.  It is an electrochemical  micro arc oxidation process for which a U.S. patent is issued on March 6, 2001.  A specimen is submerged in the electrolytic solution. A controlled high power AC current is applied to the specimen.  The specimen glows bright due to the  micro-arc created  by the surrounding plasma which creates the oxidation of the surface of the specimen. As the thickness of the coating increases, it moves inside the substrate. Practically, there is no change in the dimension of the specimen. Therefore, a completely finished part can be coated without any finishing afterward. The Microplasmic Process is also suited for a hard coating inside surface of a part i.e. a cylindrical, conical or spherical hollow parts. The Microplasmic process produces an outer soft coating of about 15 % that may be buffed off; and a remaining inner layer of extremely hard ceramic material. It creates a thick ceramic coating which exhibits excellent resistance to wear, heat and chemical corrosion.

Typical thickness 0-150+ microns. Corrosion resistant > 2000 hrs salt spray and >500 hrs in 98% sulfuric acid.

Information provided by Microplasmic Corporation.

Key Words: Anodized, New Coating, Hard Coating
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers >= 1400
Modulus of Elasticity 277 GPaYoung's Modulus
Poissons Ratio 0.21
Adhesive Bond Strength >= 7.00 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 5.00e+10 ohm-cm
Dielectric Breakdown 800 VBreak Through Voltage
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 200 W/m-K
Maximum Service Temperature, Air 1650 °Cwith cooling

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AR-Glass Fiber, Generic
Thermal Transfer Composites PRIMEX ULTRA™ MCT-487™ Aluminum Silicon Carbide Composite, Reinforced
Crystex Composites Mykroy/Mycalex 555 Molding Grade Glass-bonded Mica Composite
Crystex Composites Mykroy/Mycalex MM 411 Moldable Glass-Mica Composite
Crystex Composites Mykroy/Mycalex MM 600 Machining Grade Glass-bonded Mica Composite

CMICP1 / 1503

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.