MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Gromax CCP PBT 4815-NCB 15% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled

Material Notes: Product Description: A glass fiber 15% reinforced injection molding grade.

Characteristics:

  • Excellent electrical property
  • Excellent temperature resistance, high heat distortion temperature
  • Excellent mechanic and chemical property
  • Excellent weatherability
  • Excellent wear property
  • Excellent moldability
  • High resistance to fuels, oil, fats and many solvents

    Information provided by Gromax Enterprises Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.48 g/ccASTM D792
Moisture Absorption 0.0300 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
@Thickness 1.60 mm
horizontal; ASTM D955
 0.014 - 0.020 cm/cm
@Thickness 1.60 mm
vertical; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ASTM D785
Tensile Strength 980 kg(f)/cm²ASTM D638
Elongation at Break 3.8 %ASTM D638
Flexural Strength 142 MPaASTM D790
Flexural Modulus 55000 kg(f)/cm²ASTM D790
Izod Impact, Notched >= 6.40 kg-cm/cm
@Thickness 6.35 mm
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
Surface Resistance 1.00e+13 ohmASTM D257
Dielectric Constant 3.3
@Frequency 60 Hz
ASTM D150
Dielectric Strength 23.0 kV/mm
@Thickness 2.00 mm
ASTM D149
Dissipation Factor 0.0010
@Frequency 60 Hz
ASTM D150
Arc Resistance 90 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 55.0 µm/m-°CASTM D696
Melting Point 225 °CDSC
Deflection Temperature at 0.46 MPa (66 psi) 220 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 195 °CASTM D648
Flammability, UL94 V-0
@Thickness 0.800 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 240 - 270 °C
Nozzle Temperature 260 - 270 °C
Mold Temperature 40.0 - 120 °Csuitable temperature 60-80°C
Injection Pressure 50.0 - 120 MPa
Hold Pressure 30.0 - 80.0 MPa
Back Pressure 0.000 - 0.300 MPa
Screw Speed 60 - 120 rpmto be chosen in such a way that plasticizing time is just within cooling time
 
Descriptive Properties
Injection Ratemiddle-fast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Gromax CCP PBT 4830-BK 30% Glass Fiber Filled
Gromax PBT 4115-104D 15% Glass Fiber Filled
Gromax PBT 4130-104D 30% Glass Fiber Filled
Gromax PBT 4115-201D 15% Glass Fiber Filled
Gromax PBT 4130-201D 30% Glass Fiber Filled

PGROM037 / 147850

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.