System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Amco PRIMATOP MDPE 003937 Medium Density Polyethylene
Categories:
Polymer
;
Film
;
Thermoplastic
;
Polyethylene (PE)
;
Medium Density (MDPE)
;
Medium Density Polyethylene (MDPE), Film Grade
Material Notes:
Film, Blow Molding, Profile Extrusion. FDA 21CFR177.1520
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.937
g/cc
ASTM D1505
Melt Index of Compound
0.30
g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Film Tensile Strength at Yield, MD
3100
psi
1.0 mil; ASTM D882
Film Tensile Strength at Yield, TD
3100
psi
1.0 mil; ASTM D882
Film Elongation at Break, MD
500 %
1.0 mil; ASTM D746
Film Elongation at Break, TD
600 %
1.0 mil; ASTM D746
Elmendorf Tear Strength, MD
50.0
g/mil
1.0 mil; ASTM D1922
Elmendorf Tear Strength, TD
500
g/mil
1.0 mil; ASTM D1922
Dart Drop
130
g/mil
1.0 mil; ASTM D1790
Film Tensile Strength at Break, MD
6100
psi
1.0 mil; ASTM D882
Film Tensile Strength at Break, TD
6100
psi
1.0 mil; ASTM D882
Compliance Properties
Original Value
Comments
FDA
Yes
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Overview of materials for Medium Density Polyethylene (MDPE), Molded
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded
Bamberger Polymers Bapolene® 4022 Polypropylene, Biaxially Oriented Film Grade
Overview of materials for Low Density Polyethylene (LDPE), Molded
A. Schulman CP812 Linear, Medium-Density Polyethylene
PATOP018m / 190886
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.