MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis Borcoat™ ME0433 Polyethylene Adhesive In Powder form for Steel Pipe Coating
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Borcoat ME0433 is a maleic-anhydride grafted polyethylene polymer with excellent adhesion to fusion bonded epoxy and the top-coat HDPE.

Borcoat HE0433 is primarily designed to be used as the tie layer between epoxy corrosion protection layer and the top-coat polyethylene, which gives the physical protection of the pipe.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.934 g/ccISO 1183/ISO 1872-2B
Melt Flow 4.0 - 6.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 47ISO 868
Tensile Strength, Yield 2611 psiAt 50 mm/min; ISO 527-3
Elongation at Break >= 700 %ISO 527-3
Peel Strength >= 4.00 kN/m3-layer at 80°C; DIN 30670/NFA 49-710
 >= 15.0 kN/m3-layer; DIN 30670/NFA 49-710
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 121 °CISO 3146
Vicat Softening Point 100 °CA50 (10 N); ISO 306
Brittleness Temperature <= -80.0 °CASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BYK PRIEX® 12031 Maleic Anhydride Grafted HDPE
Borealis Borcoat™ HE3450 Black High Density Polyethylene Top Coat for Steel Pipe Coating
Borealis Borcoat™ ME0420 Grafted Polyethylene Adhesive for Steel Pipe Coating
BYK PRIEX® 11006 Maleic Anhydride Grafted HDPE
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade

PBOREA051 / 27358

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.