MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical LUTENE-H FE0070 HDPE  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: LUTENE-H FE0070 is mainly intended for the extrusion of blown film with high mechanical properties for the manufacture of "T-Shirt" grocery sacks, can liners. Especially, LUTENE-H FE0070 resin can be relied upon for excellent performance under heavy load conditions. LUTENE-H FE0070 resin is a high molecular weight, high density polyethylene. The film produced from this resin characteristically exhibits high tensile strength, stiffness, impact strength and barrier properties. It can be down-gauged to as low as 10 micro-m.

Applications: Merchandise bags, consumer trash bags, industrial and institutional liners.

CAS No. 9002-88-4

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.953 g/cc0.953 g/ccASTM D1505
Thickness 10.0 microns0.394 mil
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 37.3 MPa5410 psiASTM D822
Film Tensile Strength at Yield, TD 35.3 MPa5120 psiASTM D822
Film Elongation at Break, MD 300 %300 %ASTM D822
Film Elongation at Break, TD 500 %500 %ASTM D822
Film Tensile Strength at Break, TD 57.9 MPa8400 psiASTM D822
 
Thermal PropertiesMetricEnglishComments
Melting Point 133 °C271 °FDSC
Crystallization Temperature 133 °C271 °FMelting; DSC
Vicat Softening Point 128 °C262 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 230 °C356 - 446 °F
Blow-up Ratio (BUR) 3.0 - 5.03.0 - 5.0

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUTENE-H ME5000 HDPE
LG Chemical LUTENE-H ME9180 HDPE
Ineos T50-500-171 Polyethylene Copolymer
Formosa Plastics Formolene® LH5206 Injection Molding HDPE
ExxonMobil HD 8760.29 High Density Polyethylene Resin

PLAY200 / 148210

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.