MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Carpenter Custom 455® Stainless Steel, Condition H950 (Age Hardened 510°C)
Categories: Metal; Ferrous Metal; Stainless Steel; T 400 Series Stainless Steel

Material Notes: Data provided by Carpenter Technology Corporation.

Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory developed Custom 455® stainless, a martensitic age-hardenable stainless steel. This alloy is relatively soft and formable in the annealed condition. A single-step aging treatment develops exceptionally high yield strength with good ductility and toughness. This stainless can be machined in the annealed condition, and welded in much the same manner as other precipitation hardenable stainless steels. Because of its low work-hardening rate, it can be extensively cold formed. The dimensional change during hardening is only about -0.001 in/in, which permits close-tolerance finish machining in the annealed state. Custom 455 stainless represents a significant advancement in the area of precipitation hardening stainless steels. It should be considered where simplicity of heat treatment, ease of fabrication, high strength and corrosion resistance are required in combination.

Because of the unique combination of high strength and corrosion resistance of Custom 455 stainless there are few other alloys available for consideration. Carpenter PH13-8 Mo can be considered where good transverse toughness and ductility are necessary in large sections.

Custom 455® is a registered trademark of Carpenter Technology Corporation.

Key Words: UNS S45500
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.76 g/cc0.280 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 459459Estimated from Rockwell C for Brinell test with 3000 kg load, 10 mm ball.
Hardness, Knoop 504504Estimated from Rockwell C
Hardness, Rockwell C 4848
Hardness, Vickers 482482Estimated from Rockwell C
Tensile Strength, Ultimate 1586 MPa230000 psi
 896 MPa
@Temperature 538 °C
130000 psi
@Temperature 1000 °F
 1207 MPa
@Temperature 427 °C
175100 psi
@Temperature 801 °F
 1345 MPa
@Temperature 316 °C
195100 psi
@Temperature 601 °F
 1689 MPa
@Temperature -73.0 °C
245000 psi
@Temperature -99.4 °F
 1931 MPa
@Temperature -184 °C
280100 psi
@Temperature -299 °F
Tensile Strength, Yield 1517 MPa
@Strain 0.2 %
220000 psi
@Strain 0.2 %
 758 MPa
@Strain 0.2 %,
Temperature 538 °C
110000 psi
@Strain 0.2 %,
Temperature 1000 °F
 1124 MPa
@Strain 0.2 %,
Temperature 427 °C
163000 psi
@Strain 0.2 %,
Temperature 801 °F
 1276 MPa
@Strain 0.2 %,
Temperature 316 °C
185100 psi
@Strain 0.2 %,
Temperature 601 °F
Elongation at Break 12 %12 %In 4D
 5.0 %
@Temperature -184 °C
5.0 %
@Temperature -299 °F
 11 %
@Temperature -73.0 °C
11 %
@Temperature -99.4 °F
 12 %
@Temperature 316 °C
12 %
@Temperature 601 °F
In 4D
 14 %
@Temperature 427 °C
14 %
@Temperature 801 °F
In 4D
 18 %
@Temperature 538 °C
18 %
@Temperature 1000 °F
In 4D
Reduction of Area 50 %50 %
 20 %
@Temperature -184 °C
20 %
@Temperature -299 °F
 45 %
@Temperature -73.0 °C
45 %
@Temperature -99.4 °F
 50 %
@Temperature 316 °C
50 %
@Temperature 601 °F
 60 %
@Temperature 427 °C
60 %
@Temperature 801 °F
 70 %
@Temperature 538 °C
70 %
@Temperature 1000 °F
Modulus of Elasticity 200 GPa
@Temperature 23.0 °C
29000 ksi
@Temperature 73.4 °F
Notched Tensile Strength 793 MPa115000 psi
 1931 MPa280100 psi
 2068 MPa299900 psi
Poissons Ratio 0.30
@Temperature 23.0 °C
0.30
@Temperature 73.4 °F
Fatigue Strength 680 MPa
@# of Cycles 1.00e+7
98600 psi
@# of Cycles 1.00e+7
R.R. Moore Test, Smooth Rotating Beam
Shear Modulus 76.9 GPa
@Temperature 23.0 °C
11200 ksi
@Temperature 73.4 °F
Charpy Impact 20.0 J14.8 ft-lbV-Notch
 4.00 J
@Temperature -184 °C
2.95 ft-lb
@Temperature -299 °F
V-Notch
 14.0 J
@Temperature -73.0 °C
10.3 ft-lb
@Temperature -99.4 °F
V-Notch
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000758 ohm-cm
@Temperature 23.0 °C
0.0000758 ohm-cm
@Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.6 µm/m-°C
@Temperature 22.0 - 93.0 °C
5.89 µin/in-°F
@Temperature 71.6 - 199 °F
 11.2 µm/m-°C
@Temperature 22.0 - 260 °C
6.22 µin/in-°F
@Temperature 71.6 - 500 °F
 12.0 µm/m-°C
@Temperature 22.0 - 482 °C
6.67 µin/in-°F
@Temperature 71.6 - 900 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.050 %<= 0.050 %
Chromium, Cr 11 - 12.5 %11 - 12.5 %
Copper, Cu 1.5 - 2.5 %1.5 - 2.5 %
Iron, Fe 75 %75 %as remainder
Manganese, Mn <= 0.50 %<= 0.50 %
Molybdenum, Mo <= 0.50 %<= 0.50 %
Nb + Ta 0.10 - 0.50 %0.10 - 0.50 %
Nickel, Ni 7.5 - 9.5 %7.5 - 9.5 %
Niobium, Nb (Columbium, Cb) <= 0.50 %<= 0.50 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 0.50 %<= 0.50 %
Sulfur, S <= 0.030 %<= 0.030 %
Tantalum, Ta <= 0.50 %<= 0.50 %
Titanium, Ti 0.80 - 1.4 %0.80 - 1.4 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carpenter Custom 455® Stainless Steel, Condition H900 (Age Hardened 482°C)
Carpenter Custom 455® Stainless Steel, Condition H1000 (Age Hardened 538°C (1000°F))
Carpenter Custom 455® Stainless Steel, Annealed, 25 mm Bar
Carpenter Custom 455® Stainless Steel, Annealed, 1.27 mm Strip
Carpenter Custom 450® Stainless Steel, Condition H950 (Age Hardened 510°C)

NCAR77 / 15643

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.