MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Akrochem Naugawhite™ Technical Stabilizer
Categories: Other Engineering Material

Material Notes: Product Description: Naugawhite™ stabilizer is a non-staining antioxidant that does not discolor. It protects natural and synthetic rubbers against oxygen, light and heat. It does not yellow or pink in the presence of nitrogen dioxide showing only minor color darkening in such exposure. Naugawhite™ stabilizer is available in liquid and solid forms in three grades: Technical, Liquid and Powder.

Features:

  • Is an effective antioxidant which protects natural or synthetic rubbers against oxygen, light and heat exposures
  • Will not stain fabrics, lacquers or other materials by migration or contact
  • Available in two convenient forms
  • Liquid is easily emulsifiable for latex applications
Application:
  • For dry rubber and latex
  • Recommended for latex foam and film refrigerator gaskets, footwear, proofing, sundries, wire insulations such as SP-1 cord, automotive rubber and cloth backing compounds
  • Effective in natural rubber, synthetic polyisporene, SBR, NBR, NBR/PVC, CR, IIR.
CAS No: 7786-17-6

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.990 g/cc
 
Descriptive Properties
AppearanceViscous Amber Liquid
Content0.97Concentration of CAS 7786-17-6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH510 / 315428

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.