MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco Pyro-Tape™ 682-CR High Temperature Tape Single-layer Teflon coated fiberglass with a high strength silicone adhesive  (discontinued **)
Categories: Polymer; Adhesive; Tape

Material Notes: Applications
  • Chemical Resistance
Features
  • Teflon (DuPont registered) coated fiberglass tape
  • Chemical resistance of Teflon for corrosive environments.
  • Non-stick covering for heat seal bars and rubber molds used in the fabrication of composites.

Vendors: Aremco’s Pyro-Tape 682-Series high temperature tapes are ideal for abrasion, chemical, electrical, and thermal insulation. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Thickness 9.00 mil
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 6000 V/mil
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 500 °F
Minimum Service Temperature, Air -73.0 °C
 
Descriptive Properties
Adhesion50 oz/in
Tape Tensile Strength120 lbs/in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Standex Engraving Tribocoat® Electroless Nickel Teflon Mold Coating
Chemours Teflon® PTFE 7A Granular Molding Powder
Chemours Teflon® PTFE Grade 7B Granular Compression Molding Resin
Clariant Renol PA113G30TF15S2 Nylon 66, 30% Glass Fiber, Teflon and Silicone Lubricated
Mid-Mountain Materials ARMATEX® SRS 40 Silica Fabric Impregnated with Silicone Rubber

ZPAREM45 / 24309

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.