MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay RHODAFAC® PA23 Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Ethoxylated phosphate ester. Dispersing, wetting agent useful in suspension concentrates. Anionic emulsifier for industrial formulations. Used in a variety of applications from polyacrylamide emulsions, to pulp and paper processing, or alkaline detergents. Anti-wear and extreme pressure additive for water based metal working fluids. Good electrolyte tolerance and high stability in alkaline environement.

Identification: ETHOXYLATED FATTY ALCOHOL, PHOSPHATE ESTER

CAS: 68585 – 36 – 4

Solubility: Soluble in water, most polar and aromatic solvents.

Available in: Asia Pacific, Europe, Latin America and North America

Applications: Agrochemical formulations: Anionic dispersing and compatibility agent for SC of EC formulation. Industrial formulations: Anionic emulsifier for industrial formulations. Used in a variety of applications from polyacrylamide emulsions, to pulp and paper processing, or alkaline detergents. Good electrolyte tolerance and high stability in alkaline environment. Metal treatment: Anionic emulsifier for industrial formulations. Used in a variety of applications from polyacrylamide emulsions, to pulp and paper processing, or alkaline detergents. Good electrolyte tolerance and high stability in alkaline environment.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 80 - 8480 - 84[mg KOH/g], #1; RPG44
 125 - 135125 - 135[mg KOH/g], #2; RPG44
 
Thermal PropertiesMetricEnglishComments
Pour Point 9.00 °C48.2 °F
Flash Point >= 100 °C>= 212 °F
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 1.0<= 1.0RPG18
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceClear to cloudy liquid
CompositionActive1
Ionic ChargeAnionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay RHODAFAC® RS-610 Surfactant
Solvay RHODAFAC® RS-410 Surfactant
Solvay RHODAFAC® PA32 Surfactant
Solvay RHODAFAC® PA15 Surfactant
Solvay RHODAFAC® BN-936/S Surfactant

WRHOD359 / 137590

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.