MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient Elastamax™ HTE 3060 Polyvinyl Chloride + NBR (PVC+NBR)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Elastamax™ HTE Series thermoplastic elastomers (TPEs) are based upon compounded blends of PVC resins and nitrile rubber. These elastomeric materials provide outstanding resistance to hydrocarbons and oils, offer excellent weatherability, and are an economical alternative to thermoset rubber and other more costly thermoplastic elastomers.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/ccASTM D792
Melt Flow 26 g/10 min
@Load 5.00 kg,
Temperature 190 °C
Procedure A; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 5915 sec; ASTM D2240
Tensile Strength at Break 14.0 MPaType IV, 510 mm/min; ASTM D638
Tensile Stress at Strain 3.74 MPa
@Strain 100 %
Type IV, 510 mm/min; ASTM D638
 8.85 MPa
@Strain 300 %
Type IV, 510 mm/min; ASTM D638
Elongation at Break 460 %Type IV, 510 mm/min; ASTM D638
Tear Strength 30.1 kN/mDie C, 510 mm/min; ASTM D624
Compression Set 49 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395A
 58 %
@Temperature 100 °C,
Time 79200 sec
ASTM D395A
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -59.0 °CASTM D746
 
Descriptive Properties
AppearanceNatural Color
FeaturesGeneral Purpose
FormsPellets
Generic MaterialPVC+NBR
Generic NamePolyvinyl Chloride + NBR (PVC+NBR)
Processing MethodExtrusion
 Injection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAutomotive Applications
 Construction Applications
 General Purpose
 Industrial Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Flexible XV3878G Polyvinyl Chloride + NBR (PVC+NBR)
Geon® Performance Solutions Vinyl Flexible R277AM Polyvinyl Chloride + NBR (PVC+NBR)
Geon® Performance Solutions Vinyl Flexible R263AM Polyvinyl Chloride + NBR (PVC+NBR)
Geon® Performance Solutions Vinyl Flexible R252BE Polyvinyl Chloride + NBR (PVC+NBR)
Geon® Performance Solutions Vinyl Flexible R252AE Polyvinyl Chloride + NBR (PVC+NBR)

PH0POL0455 / 145024

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.