MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC CYCOLAC™ MG38N ABS (Asia)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccASTM D792
Viscosity 2450 cP
@Shear Rate 1000 1/s,
Temperature 240 °C
melt; ASTM D3825
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 3.7 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 15 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 34.0 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 45.0 MPa5 mm/min; ASTM D638
Elongation at Break 26 %5 mm/min; ASTM D638
Elongation at Yield 2.1 %5 mm/min; ASTM D638
Tensile Modulus 2270 MPa5 mm/min; ASTM D638
Flexural Yield Strength 72.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2340 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 374 J/mASTM D256
Dart Drop, Total Energy 31.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 120 - 180 secASTM D495
Comparative Tracking Index >= 600 VUL 746A
Hot Wire Ignition, HWI 15 - 30 secUL 746A
High Amp Arc Ignition, HAI >= 120 arcsUL 746A
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 88.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 86.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 99.0 °CRate B/50; ASTM D1525
UL RTI, Electrical 60.0 °CUL 746B
UL RTI, Mechanical with Impact 60.0 °CUL 746B
UL RTI, Mechanical without Impact 60.0 °CUL 746B
Flammability, UL94 HB
@Thickness 1.52 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 220 - 260 °CInjection Molding
Zone 1 190 - 210 °C
Zone 2 205 - 225 °C
Zone 3 215 - 240 °C
Melt Temperature 220 - 260 °C
Mold Temperature 50.0 - 70.0 °C
Drying Temperature 80.0 - 95.0 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Moisture Content 0.10 %
Back Pressure 0.300 - 0.700 MPa
Shot Size 50 - 70 %
Vent Depth 0.00380 - 0.00510 cm
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10092 / 243559

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.