MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Reynolds Formlastic™ 48 Urethane
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Formlastic™ 60 urethane is a durable mold rubber made for production casting of concrete. It features a low viscosity for easy mixing and pouring and cures with minimal bubble entrapment. Mix ratio is 1A:1B by volume, pot life is 40 minutes and the rubber cures with an ultimate Shore hardness of Shore 60A. Cured rubber is dimensionally stable (low shrinkage), offers good wear resistance and will render color accurate concrete castings.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.14 g/ccASTM D-1475
Linear Mold Shrinkage <= 0.0010 in/in
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 48ASTM D-2240
Tensile Strength 700 psiASTM D-412
Elongation at Break 1250 %ASTM D-412
Tear Strength 98.0 pliDie C; ASTM D-624
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hour
Pot Life 25.0 minASTM D-2471
 
Descriptive Properties
ColorOff-White
Mix Ratio100A:118Bby weight
 1A:1Bby volume
Specific Volume24.3[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREYN094 / 296795

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.